热处理工艺对PH13-8Mo钢的组织和性能的影响Effect of heat treatment process on microstructure and properties of PH13-8Mo steel
程志伟,金建军,鲁世强,胡春文,刘大博,刘俊伟
摘要(Abstract):
利用光学显微镜、透射电子显微镜和力学性能测试,研究了不同淬火温度(850~1050℃)和回火温度(100~750℃)对PH13-8Mo钢微观组织和力学性能的影响。结果表明,经过淬火后形成的含有高密度位错的细小板条马氏体是该钢具有较高强韧性的组织基础,在500℃左右回火时,与基体共格的细小弥散分布的NiAl沉淀相是该钢出现强度峰值的主要原因。NiAl沉淀相在450℃左右回火时开始析出,高于510℃回火时因NiAl相长大而逐渐与基体失去共格关系,高于700℃回火时NiAl相溶解。PH13-8Mo钢经925℃淬火和510℃回火可获得良好的综合性能。
关键词(KeyWords): PH13-8Mo钢;NiAl沉淀相;微观组织;热处理;性能
基金项目(Foundation): 国家自然科学基金(51164030)
作者(Author): 程志伟,金建军,鲁世强,胡春文,刘大博,刘俊伟
DOI: 10.13289/j.issn.1009-6264.2013.11.010
参考文献(References):
- [1]孙永庆,杨志勇,梁剑雄,等.中国商用飞机高强度不锈钢的现状及发展趋势[J].钢铁研究学报,2009,21(6):1-5.SUN Yong-qing,YANG Zhi-yong,LIANG Jian-xiong,et al.Progress and prospect of high strength stainless steel for civil airplanes in China[J].Journal of Iron and Steel Research,2009,21(6):1-5.
- [2]刘振宝,宋为顺,杨志勇,等.时效对超高强马氏体时效不锈钢组织与性能的影响[J].材料热处理学报,2005,26(4):52-55.LIU Zhen-bao,SONG Wei-shun,YANG Zhi-yong,et al.The effect of aging on microstructure and properties for ultra-high strength martensite stainless steel[J].Transactions of Materials and Heat Treatment.2005,26(4):52-55.
- [3]Liu R L,Yan M F.The microstructure and properties of 17-4PH martensitic precipitation hardening stainless steel modified by plasma nitrocarburizing[J].Surface and Coatings Technology,2010,204(14):2251-2256.
- [4]杨世伟,夏德贵,杨晓,等.调整处理对17-4PH不锈钢耐海水腐蚀性能的影响[J].材料热处理学报,2007,28(增刊):184-187.YANG Shi-wei,XIA De-gui,YANG Xiao,et al.Effect of intermediate treatment on seawater corrosion resistance property of 17-4PH stainless steel[J].Transactions of Materials and Heat Treatment,2007,28(S):184-187.
- [5]Abdelshehid M,Mahmodieh K,Mori K,et al.On the correlation between fracture toughness and precipitation hardening heat treatments in 15-5PH Stainless Steel[J].Engineering Failure Analysis,2007,14(4):626-631.
- [6]Xu X L,Yu Z W.Metallurgical analysis on a bending failed pump-shaft made of 17-7PH precipitation-hardening stainless steel[J].Journal of Materials Processing Technology,2008,198(1-3):254-259.
- [7]陈国辉,张小聪,罗承萍,等.沉淀硬化不锈钢PH15-7Mo的时效行为[J].金属热处理,2010,35(7):54-57.CHEN Guo-hui,ZHANG Xiao-cong,LUO Cheng-ping,et al.Aging behavior of PH15-7Mo precipitation-hardening stainless steel[J].Heat Treatment of Metals,2010,35(7):54-57.
- [8]Seetharaman V,Sundararaman M,Krishnan R.Precipitation hardening in a PH 13-8 Mo stainless steel[J].Materials Science and Engineering,1981,47(1):1-11.
- [9]刘天琦,支敏学,朱杰远,等.热处理制度对0Cr13Ni8Mo2Al钢组织和性能的影响[J].材料工程,2002(5):26-29.LIU Tian-qi,ZHI Min-xue,ZHU Jie-yuan,et al.Effect of heat treatment on microstructure and mechanical properties of 0Cr13Ni8Mo2Al steel[J].Journal of Materials Engineering,2002(5):26-29.
- [10]Sato K.Improving the Toughness of Ultrahigh Strength Steel[D].University of California Berkeley,2002.
- [11]中国航空材料手册编辑委员会.中国航空材料手册:结构钢,不锈钢[M].北京:中国标准出版社,2002.
- [12]舒小勇,鲁世强,刘大博,等.0Cr13Ni8Mo2Al钢在900~1050℃时的变形组织演变规律研究[J].热加工工艺,2011,40(8):13-16.SHU Xiao-yong,LU Shi-qiang,LIU Da-bo,et al.Investigation on deformation microstructure evolution of 0Cr13Ni8Mo2Al steel at 900-1050℃[J].Hot Working Technology,2011,40(8):13-16.
- [13]舒小勇,鲁世强,郑海忠,等.应变对PH13-8Mo钢在1050~1150℃时变形组织的影响[J].宇航材料工艺,2011,41(5):69-73.SHU Xiao-yong,LU Shi-qiang,ZHENG Hai-zhong,et al.Effect of strain on microstructure evolution of PH13-8Mo steel deformed at 1050 to 1150℃[J].Aerospace Materials&Technology,2011,41(5):69-73.
- [14]孙志华,张晓云,汤智慧,等.马氏体沉淀硬化不锈钢0Cr13Ni8Mo2Al的腐蚀性能[J].腐蚀与防护,2006,27(12):629-631.SUN Zhi-hua,ZHANG Xiao-yun,TANG Zhi-hui,et al.Corrosion properties of 0Cr13Ni8Mo2Al stainless steel[J].Corrosion&Protection,2006,27(12):629-631.
- [15]Pape J A,Neu R W.Fretting fatigue damage accumulation in PH13-8Mo stainless steel[J].International Journal of Fatigue,2001,23:437-444.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||