S30432耐热钢650℃时效的组织和力学性能Microstructure and mechanical properties of S30432 heat-resistant steel aged at 650℃
张玉洁,杨函,朱丽慧
摘要(Abstract):
研究了S30432耐热钢在650℃时效时的微观组织和力学性能,特别探讨了S30432钢时效过程中析出相的变化对力学性能的影响。结果表明,实验合金时效初期ε-Cu和M23C6大量析出,随后逐渐长大,其中M23C6尺寸较大且粗化较快,但ε-Cu长期时效后尺寸依然细小。时效初期硬度升高的主要原因是ε-Cu的析出,长期时效过程中ε-Cu尺寸保持细小是硬度稳定在较高水平的主要原因。此外,时效初期由于M23C6大量析出冲击韧性急剧下降,随后M23C6的粗化是冲击韧性继续下降的主要原因。
关键词(KeyWords): S30432耐热钢;时效;组织;力学性能;ε-Cu
基金项目(Foundation): 上海市教育委员会科研创新项目(09YZ26);; 上海大学研究生创新基金资助项目(SHUCX102231)
作者(Author): 张玉洁,杨函,朱丽慧
DOI: 10.13289/j.issn.1009-6264.2011.03.019
参考文献(References):
- [1]Muramatsu K.Advanced Heat Resistant Steel for Power Generation[M].Cambridge:The University Press,1999.
- [2]Fujio Abe.Precipitate design for creep strengthening of 9%Cr tempered martensitic steel for ultra-supercritical power plants[J].Sci Technol AdvMater,2008,9:1-15.
- [3]Masaaki Igarashi.Long-term creep characteristics of advanced hear-resistant stainless steels for fossil fired power plant boilers[J].CAMP-ISIJ,2004,17:336-339.
- [4]Sourmail T.Precipitation in creep resistant austenitic stainless steels[J].Mater Sci Technol,2001,17:1-14.
- [5]Kota Sawada,Hideaki Kushima,Kazuhiro Kimura.Z-phase formation during creep and aging in 9-12%Cr heat resistant steels[J].ISIJ Int,2006,46(5):769-775.
- [6]Yuichi Futamura,Toshihiro Tsuchiyama,Setsuo Takaki.Strengthening mechanism of Cu bearing heat resistant martensitic steels[J].ISIJ Int,2001,41:S106-S110.
- [7]Hideto Kimura.Precipitation behavior and 2-step aging of 17-4PH stainless steel[J].J Iron Steel Inst,2000,86:343-348.
- [8]Dieter Isheim R,Prakash Kolli,Morris E Fine,et al.An atom-probe tomographic study of the temporal evolution of the nanostructure of Fe-Cu basedhigh-strength low-carbon steels[J].Scripta Materialia,2006,55:35-40.
- [9]Fukuya K,Ohno K,Nakata H,et al.Microstructural evolution in medium copper low alloysteels irradiated in a pressurized water reactor and amaterial test reactor[J].Journal of Nuclear Materials,2003,312:163-173.
- [10]Dieter Isheim,Semyon Vaynman,Morris E Finea,et al.Copper-precipitation hardening in a non-ferromagnetic,face-centered cubic austenitic steel[J].Scripta Materialia,2008,59:1235-1238.
- [11]Gür C H,Ylldlz I.Non-destructive investigation on the effect of precipitation hardening on impact toughness of 7020 Al-Zn-Mg alloy[J].Mater SciEng A,2004,382:395-400.
- [12]Saucedo-Munoz M L,Watanabe Y,Tetsuo Shoji,et al.Effect of microstructure evolution on fracture toughness in isothermally aged austeniticstainless steels for cryogenic applications[J].Cryogenics,2000,40:693-700.
- [13]Guan K,Xu X D,Xu H,et al.Effect of aging at 700℃on precipitation and toughness of AISI321 and AISI347 austenitic stainless steel welds[J].Nuclear Engineering and Design,2005,235:2485-2494.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||