La3+掺杂Y2O3透明陶瓷制备及发光性能Fabrication of Y2O3 doped with La3+ transparent ceramics and luminescence properties
罗军明,邓莉萍,艾云龙,温祯洪
摘要(Abstract):
以Y2O3为基质材料,掺杂不同含量的La3+,采用机械力化学法制备纳米粉,粉体压制后在真空度1×10-3Pa下烧结得到La3+掺杂Y2O3透明陶瓷。采用透射电子显微镜(TEM)观察粉体一次颗粒形貌,扫描电镜(SEM)观察样品表面形貌,HV-1000型维氏硬度计测定样品硬度和断裂韧性,阿基米德法测定烧结后试样的相对密度,自动记录分光光度计测定试样透过率。结果表明:制备的La3+∶Y2O透明陶瓷透光率可达80%,掺杂La3+可以显著降低La3+∶Y2O3透明陶瓷的烧结温度;随着La2O3添加量的提高,样品透光率逐渐提高,但La2O3添加量过大会造成点阵畸变严重;随着La2O3添加量的提高,样品相对密度、维氏硬度和断裂韧性均逐渐提高,最后趋于平稳;随着保温时间延长,样品透光率也逐渐增大,继续增大保温时间,透光率趋于平缓。结合样品的透光率、相对密度、维氏硬度和断裂韧性考虑可知La2O3适合掺杂量、烧结温度和保温时间分别为10at%、1550℃和3h。
关键词(KeyWords): La3+掺杂Y2O;透明陶瓷;机械力化学法
基金项目(Foundation): 航空科学基金(2008ZF56010);; 江西省自然科学基金(2007GZC1553);; 江西省教育厅科研项目(GJJ09199);; 南昌航空大学科研基金(EA200901029)
作者(Author): 罗军明,邓莉萍,艾云龙,温祯洪
DOI: 10.13289/j.issn.1009-6264.2010.03.001
参考文献(References):
- [1]Lu J,Prabhu M,Song J,et al.Optical properties and highly efficient laserosciuation of Nd3+:YAG ceramics[J].Appl Phys B,2000,71(4):469-473.
- [2]Daisuke M.Highly efficient continuous wave operation at1030and1075nm wavelengths of LD pumped Yb3+∶Y2O3ceramic lasers[J].Appl Phys lett,2004,84(3):317-319.
- [3]闻雷,孙旭东,其鲁,等.湿化学法制备Y2O3纳米粉及透明陶瓷[J].无机材料学报,2006,21(3):539-546.WEN Lei,SUN Xu-dong,QI Lu,et al.Solution-based proeessingof Y2O3nano Powders yielding transparent ceramics[J].Journal of Inorganic Materials,2006,21(3):539-546.
- [4]罗军明,李永绣,邓莉萍.共沉淀法制备Er3+:Y2O3上转换发光纳米粉[J].稀有金属材料与工程,2007(8):1436-1439.LUO Jun-ming,LI Yong-xiu,DENG Li-ping.Fabrication of Er3+∶Y2O3nanocrystalline powder of upconversion luminescence by co-precipitation method[J].Rare Metal Materials and Engineering,2007(8):1436-1439.
- [5]Wu N Q,Su L Z,Yuan M Y,et al.Preparation and microstructure of nano-sized Cu particles by mechanochemical reaction[J].Transaction of Nonferrous Metal Soc of China,1998,8(4):610-612.
- [6]Li Y X,Zhou X Z,Wang Z Q.Mechanochemical reaction between lanthanum carbonate and sodium hydroxide and the preparation of lanthanum oxide nanoparticle[J].J.Rare Earths,2002,20(5):411-445.
- [7]Li Y X,Zhou X Z,Wang Y,et al.Preparation of nano-sized CeO2by the mechanochemical reaction of cerium carbonate with sodium hydroxide[J].Mater Lett,2004,58(1-2):245-248.
- [8]辜子英,胡平贵,彭德院,等.单分散球形超细氧化铈的机械化学反应制备法[J].中国有色金属学报,2003,13(3):787-790.GU Zi-ying,HU Ping-gui,PENG De-yuan,et al.Preparation of monodisperse spherical superfine cerium dioxide using mechanochemical method[J].The Chinese Journal of Nonferrous Metals,2003,13(3):787-790.
- [9]刘军芳,傅正义,张东明,等.透明陶瓷的制备技术及其透光因素的研究[J].硅酸盐通报,2003(3):68-72.LIU Jun-fang,FU Zheng-yi,ZHANG Dong-ming,et al.Study on the preparation techniques for transparent ceramics and its transmissivity factors[J].Bulletin of the Chinese Cerrmic Society,2003(3):68-72.
- [10]杨秋红,徐军,苏良碧.Yb:Y2-2xLa2XO3激光透明陶瓷的光谱性能[J].物理学报,2006,55(3):1208-1210.YANG Qiu-hong,XU Jun,SU Liang-bi.Spectroscopic characteristics of transparent Yb:Y2-2xLa2xO3laser ceramics[J].Acta Physica Sinica,2006,55(3):1208-1210.
- [11]Ikesue A,Yoshida K.Infuence of pore volume on laser performance of Nd:YAG ceramics[J].J Mat Sci,1999,34(6):1189-1195.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||