微量氢对电子束焊接Ti-6Al-4V钛合金疲劳寿命的影响Effect of hydrogen on fatigue behavior of electron beam welded Ti-6Al-4V alloy
籍龙波,胡树兵,李行志,王亚军,陈冀彦,肖建中
摘要(Abstract):
对Ti-6Al-4V钛合金电子束焊接试样进行高温气体渗氢,研究了置氢对显微组织形态的影响,并对微量氢对Ti-6Al-4V疲劳寿命的影响进行考察。显微组织研究结果表明:置氢浓度低于0.120 wt%时,氢以固溶态存在于合金中,并未形成氢化物;位错在次生的α、β相区聚集,α/β相界往往是裂纹萌生的根源。疲劳实验结果表明:随置氢浓度的增加,疲劳寿命大幅下降;这是由于微量氢的存在降低了Ti-6Al-4V的韧性,并加速疲劳裂纹的扩展,从而降低了疲劳寿命。
关键词(KeyWords): Ti-6Al-4V;电子束焊接;氢;疲劳寿命
基金项目(Foundation): 华中科技大学材料成形与模具技术国家重点实验室基金项目(09-10);; 2010年省部产学研合作重大项目(2010A090200047);; 国家磁约束核聚变能研究专项(2010GB109000)
作者(Author): 籍龙波,胡树兵,李行志,王亚军,陈冀彦,肖建中
DOI: 10.13289/j.issn.1009-6264.2011.06.023
参考文献(References):
- [1]Tal-Gutelmacher E,Eliezer D,Eylon D.The effects of low fugacity hydrogen in duplex-and beta-annealed Ti-6Al-4V alloy[J].Materials Science andEngineering A,2004,A381(1-2):230-236.
- [2]Taha A,Sofronis P.A micromechanics approach to the study of hydrogen transport and embrittlement[J].Engineering Fracture Mechanics,2001,68(6):803-837.
- [3]Liu H,Cao J,He P,et al.Effect of hydrogen on diffusion bonding of commercially pure titanium and hydrogenated Ti6Al4V alloys[J].InternationalJournal of Hydrogen Energy,2009,34(2):1108-1113.
- [4]Luo L S,Su Y Q,Guo J J,et al.Formation of titanium hydride in Ti-6Al-4V alloy[J].Journal of Alloys and Compounds,2006,425(1-2):140-144.
- [5]Shan D B,Zong Y Y,Lv Y,et al.The effect of hydrogen on the strengthening and softening of Ti-6Al-4V alloy[J].Scripta Materialia,2008,58(6):449-452.
- [6]Zhu T K,Li M Q.Effect of 0.770wt%H addition on the microstructure of Ti-6Al-4V alloy and mechanism ofδhydride formation[J].Journal of Alloysand Compounds,2009,481(1-2):480-485.
- [7]Boyer R R,Spurr W F.Characteristics of sustained-load cracking and hydrogen effects in Ti-6Al-4V[J].Metallurgical Transactions A,1978,9(1):23-29.
- [8]Moody N R,Gerberich W W.Effect of stress state on internal hydrogen-induced crack growth in Ti-6Al-6V-2Sn[J].Metallurgical Transactions A,1982,13(6):1055-1061.
- [9]Shih D S,Robertson I M,Birnbaum H K.Hydrogen embrittlement of alpha titanium:in situ TEM studies[J].Acta Metallurgica,1998,36(1):111-124.
- [10]李晓华,侯红亮,李志强.置氢Ti6Al4V合金的微观组织演变规律[J].材料科学与工艺,2009,17(3):185-388.LI Xiao-hua,HOU Hong-liang,LI Zhi-qiang.Microstructure transition of hydrogenated Ti6Al4V alloy[J].Materials Science and Technology,2009,17(3):185-388.
- [11]何晓,沈保罗,岳俊,等.氢对Ti-2Al-2.5Zr钛合金疲劳性能的影响[J].金属热处理,2002,27(12):10-13.HE Xiao,SHEN Bao-luo,YUE Jun,et al.Effects of hydrogen on fatigue property for Ti-2Al-2.5Zr titanium alloy[J].Heat Treatment of Metals,2002,27(12):10-13.
- [12]李晓华,孙中刚,侯红亮,等.置氢Ti-6Al-4V合金组织与室温变形行为的相关性[J].北京科技大学学报,2008,30(8):888-892.LI Xiao-hua,SUN Zhong-gang,HOU Hong-liang,et al.Correlation between microstructure and room-temperature deformation behavior of thehydrogenated Ti-6Al-V alloy[J].Journal of University of Science and Technology Beijing,2008,30(8):888-892.
- [13]郭隆,白秉哲,侯红亮.置氢Ti-6Al-4V钛合金超塑性研究[J].稀有金属,2009,33(4):467-471.GUO Long,BAI Bing-zhe,HOU Hong-liang.Superplasticity of Ti-6Al-4V alloy processed by hydrogenation[J].Chinese Journal of Rare Metals,2009,33(4):467-471.
- [14]Thompson N,Wadsworth N J,Louat N.The origin of fatigue fracture in copper[J].Philosophical Magazine,1956,1(2):113-126.
- [15]Senkov O N,Jonas J J.Effect of phase composition and hydrogen level on the deformation behavior of titanium-hydrogen alloys[J].Metall and MaterTrans A,1995,27(7):1869-1876
- [16]Senkov O N,Jonas J J.Dynamic strain aging and hydrogen-induced softening in alpha titanium[J].Metall and Mater Trans A,1996,27(7):1877-1887.
- [17]Castany P,Pettinari-Sturmel F,Crestou J,et al.Experimental study of dislocation mobility in a Ti-6Al-4V alloy[J].Acta Materialia,2007,55(18):6284-6291.
- [18]Williams D P,Nelson H G.Gaseous hydrogen-induced cracking of Ti-5Al-2.5Sn[J].Metall and Mater Trans,1972,3(8):2107-2113.
- [19]Pao P S,Feng C R,Gill S J.Hydrogen-assisted fatigue crack growth in beta-annealed Ti-6Al-4V[J].Scripta Materialia,1998,40(1):19-26.
- [20]何晓.含氢的新型钛合金的疲劳行为研究[D].四川:四川大学,2003.
- [21]唐志平,彭楚峰,何晓,等.氢对Ti-2Al-2.5Zr钛合金疲劳裂纹扩展速率的影响[J].核动力工程,2003,24(6):555-558.TANG Zhi-ping,PENG Chu-feng,HE Xiao,et al.Effects of hydrogen on fatigue crack propagation rate of Ti-2Al-2.5Zr titanium alloy[J].NuclearPower Engineering,2003,24(6):555-558.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||