AL6XN奥氏体钢的时效析出研究Study of precipitation in AL6XN austenitic steel at elevated temperatures
孟丽君,邢辉,孙坚
摘要(Abstract):
采用电子显微术对AL6XN奥氏体不锈钢在500~750℃经过最长3600 h时效后的析出进行研究。结果显示,试验钢在500~550℃没有析出物产生;在600℃时效后,奥氏体晶界析出碳化物。当温度升高到650~750℃,大量的析出物出现在奥氏体晶界以及晶粒内部,通过选区电子衍射及能谱分析表明AL6XN奥氏体钢的析出物为σ与Laves相的金属间化合物。
关键词(KeyWords): AL6XN奥氏体钢;碳化物;σ相;Laves相;析出
基金项目(Foundation): 国家重点基础研究发展计划(973)项目(2007CB209803);; 上海市科委技术创新服务平台课题(10DZ2290904)
作者(Author): 孟丽君,邢辉,孙坚
DOI: 10.13289/j.issn.1009-6264.2011.05.017
参考文献(References):
- [1]朱发文,张乐福,乔培鹏,等.超临界水堆候选材料的腐蚀特性研究[J].核动力工程,2009,30(5):62-66.Zhu F W,Zhang L F,Qiao P P,et al.Corrosion behaviors of candidate materials for supercritical-cooled water reactor[J].Nuclear Power Engineering,2009,30(5):62-66.
- [2]Borst K,Pohl M.Precipitation effects in austenitic stainless weld metals[J].Materials Technology,1990,6:258-261.
- [3]Kunimitsu S,Iwamoto T,Hotta A,et al.Effect of Mo and Si on Laves phase precipitation in 10%Cr-steels[C]//Proc Int Conf on Stainless Steels,Chiba ISIJ,1991:627-632.
- [4]郭伟国.4种新型舰艇钢的塑性流变应力及其本构模型[J].金属学报,2006,42(5):463-468.Guo W G.Plastic flow stresses and constitutive models of four newer naval vessel steels[J].Acta Metallurgica Sinica,2006,42(5):463-468.
- [5]Meng L J,Sun J,Xing H,et al.Serrated flow behavior in AL6XN austenitic stainless steel[J].Journal of Nuclear Materials,2009,394:34-38.
- [6]孟丽君,邢辉,庞淦文,等.AL6XN超级奥氏体钢高温蠕变及疲劳行为研究[J].原子能科学技术,2009,43(6):509-513.Meng L J,Xing H,Pang G W,et al.High-temperature creep and fatigue behaviors of AL6XN super austenite steel[J].Atomic Energy Science andTechnology,2009,43(6):509-513.
- [7]孟丽君,庞淦文,邢辉,等.AL6XN超级奥氏体钢高温拉伸时的动态应变时效[J].材料热处理学报,2010,31(4):50-54.Meng L J,Pang G W,Xing H,et al.Dynamic strain aging effect during high-temperature tensile test of AL6XN super austenite steel[J].Transactionsof Materials and Heat Treatment,2010,31(4):50-54.
- [8]Beckitt F R,Clark B R.The shape and mechanism of formation of M23C6 carbide in austenite[J].Acta Metallurgica,1967,15(1):113-129.
- [9]Lo I H,Tsai W T.Effect of heat treatment on the precipitation and pitting corrosion behavior of 347SS weld overlay[J].Materials Science andEngineering A,2003,355:137-143.
- [10]Brun G,Le Naour J,Vouillon M.Etude de la microstructure d'un acier 316 titane apres vieillissement et apres irradiation aux neutrons[J].Journal ofNuclear Materials,1981,1-2:109-123.
- [11]Williams T M.Precipitation in neutron-irradiated type 316 austenitic steel[C]//Stainless steels 84,Inst of Metals(Book n 320),London,England,1985.
- [12]Takahashi Y,Shibamoto H,Inoue K.Long-term creep rupture behavior of smoothed and notched bar specimens of low-carbon nitrogen-controlled 316stainless steel(316FR)and their evaluation[J].Nuclear Engineering and Design,2008,238(2):310-321.
- [13]Weiss B,Stickler R.Phase instabilities during high temperature exposure of 316 austenitic stainless steel[J].Metallurgical and Materials TransactionsA,1972,3(4):851-866.
- [14]Jargelius-Petterson R F A.Precipitation trends in highly alloyed austenitic stainless steels[J].Materials Research and Advanced Techniques,1998,79:177-183.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||