基于Murty判据的TB8钛合金加工图及变形区分析Processing map and deformation zone analyses of TB8 titanium alloy based on Murty criterion
袁大庆,董洪波,邹忠波,徐远刚
摘要(Abstract):
采用Gleeble3500对TB8钛合金进行等温恒应变速率热模拟压缩试验,研究该合金在温度750~900℃、应变速率0.001~10 s-1热变形参数范围内基于Murty判据的加工图,并分析TB8钛合金的热变形行为。结果表明:TB8钛合金的失稳变形区为:温度750~780℃,应变速率0.03~10 s-1;温度780~900℃,0.35~10 s-1,发生失稳变形后的组织特征为局部流动及β相晶粒的不均匀变形。较佳的稳定变形区为:温度815~885℃、应变速率0.03~0.1 s-1,发生稳定变形后的组织为动态再结晶后的等轴组织。结合预测的稳定变形区及显微组织特征可知,在单相区850℃变形时,0.1 s-1作为动态回复及动态再结晶的临界应变速率。
关键词(KeyWords): TB8钛合金;Murty判据;加工图;变形区
基金项目(Foundation): 航空科学基金项目(2015ZE56011);; 江西省科学计划项目(20151BBE50042)
作者(Author): 袁大庆,董洪波,邹忠波,徐远刚
DOI: 10.13289/j.issn.1009-6264.2016.11.013
参考文献(References):
- [1]董显娟,鲁世强,王克鲁,等.基于Prasad判据的全片层TA15钛合金塑性流动失稳预测[J].航空材料学报,2010,30(2):11-16.DONG Xian-juan,LU Shi-qiang,WANG Ke-lu,et al.Prediction of plastic flow instability of TA15 titanium alloy with full lamellar based on prasad criterion[J].Journal of Aeronautical Materials,2010,30(2):11-16.
- [2]李鑫,鲁世强,王克鲁,等.基于Murty准则粗片层TC11合金两相区的热态变形行为[J].中国有色金属学报,2008,18(8):1407-1413.LI Xin,LU Shi-qiang,WANG Ke-lu,et al.Hot deformation behavior of TC11 alloy with thick lamellar microstructure in two phase field based on Murty criterion[J].The Chinese Journal of Nonferrous Metals,2008,18(8):1407-1413.
- [3]Tal-Gutelmacher E,Eliezer D,Boellinghaus Th.Investigation of hydrogen-deformation interactions inβ-21S titanium alloy using thermal desorption spectroscopy[J].Journal of Alloys and Compounds,2007,440(12):204-209.
- [4]Berger M C,Gregory J K.Residual stress relaxation in shot peened timetal 21s[J].Materials Science and Engineering A,1999,263(2):200-204.
- [5]Mohan L,Anandan C,Grips V K W.Corrosion behavior of titanium alloy Beta-21S coated with diamond like carbon in Hank's solution[J].Applied Surface Science,2012,258(17):6331-6340.
- [6]Tang B,Tang B,Han F,et al.Hot deformation behavior of TB8 alloy near theβ-Transus[J].Rare Metal Materials and Engineering,2013,42(9):1761-1766.
- [7]周晓虎,马文革,俞汉清,等.TB8超高强度钛合金热工艺参数研究[J].材料工程,2003(8):37-39.ZHOU Xiao-hu,MA Wen-ge,YU Han-qing,et al.Thermo-mechanical processing parameters of TB8 super-high strength titanium alloy[J].Journal of Materials Engineering,2003(8):37-39.
- [8]刘诚,董洪波,张贵华,等.基于Murty判据的TC4-DT合金加工图及失稳分析[J].锻压技术,2015,40(1):113-118.LIU Cheng,DONG Hong-bo,ZHANG Gui-hua,et al.Processing drawing and flow instability analysis of TC4-DT titanium alloy based on Murty criterion[J].Forging and Stamping Technology,2015,40(1):113-118.
- [9]Murty S V S N,Rao B N,Kashyap B P.Instability criteria for hot deformation of materials[J].International Materials Reviews,2000(1):15-26.
- [10]戚运莲.Ti600高温钛合金的热变形行为及加工图研究[D].西安:西北工业大学,2007.QI Yun-lian.Study on hot deformation behavior and processing map of high temperature titanium alloy Ti600[D].Xi'an:Northwestern Polyteehnieal University,2007.
- [11]王克鲁,鲁世强,康永林,等.Ti3Al基合金的热变形行为及加工图[J].稀有金属材料与工程,2011,40(9):1534-1539.WANG Ke-lu,LU Shi-qiang,KANG Yong-lin,et al.Deformation behavior and processing map of Ti3Al based alloy during the isothermal compression[J].Rare Metal Materials and Engineering,2011,40(9):1534-1539.
- [12]王克鲁,鲁世强,董显娟,等.Ti-6.5Al-3.5Mo-1.5Zr-0.3Si合金绝热剪切和局部流动行为[J].航空学报,2009,30(10):1967-1972.WANG Ke-lu,LU Shi-qiang,DONG Xian-juan,et al.Behavior of adiabatic shear and flow localization of alloy Ti-6.5Al-3.5Mo-1.5Zr-0.3Si[J].Acta Aeronautica et Astronautica Sinica,2009,30(10):1967-1972.
- [13]张利军,周中波,常辉,等.高钼含量β型钛合金的偏析行为及预防措施[J].中国有色金属学报,2013(8):2206-2212.ZHANG Li-jun,ZHOU Zhong-bo,CHANG Hui,et al.Segregation behavior and prevention measures of beta titanium alloy with high molybdenum content[J].The Chinese Journal of Nonferrous Metals,2013(8):2206-2212.
- [14]胡赓祥,蔡珣,戎咏化,等.材料科学基础[M].上海:上海交通大学出版社,2010.HU Sai-xiang,CAI Xun,RONG Yong-hua,et al.Fundamentals of Materials Science[M].Shanghai:Shanghai Jiao Tong University Press,2010.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||