摘要(Abstract):
将含Cu高硅钢薄板退火后,以不同方式冷却,通过微观组织观察、织构分析以及磁性能测量,研究了冷却速度对含Cu高硅钢再结晶组织、织构及磁性能的影响。结果表明,冷却速度对再结晶组织几乎没有影响,但冷却速度减慢会提高{100}面织构的含量,降低{110}和{111}面织构的含量;0.4Cu试样的晶粒尺寸略大于0.2Cu试样,不同Cu含量试样织构组分差异不大;冷却速度和Cu含量共同作用下,冷却速度对高硅钢磁性能的影响占主导因素。冷却速度越慢,织构因子越大,磁感越高,{100}面织构含量越高,残余应力越小,并且高硅钢中长程有序度越高,有序相的反相畴尺寸越大,这些因素都有利于降低铁损。
关键词(KeyWords): 含Cu高硅钢;冷却速度;组织;织构;磁性能
基金项目(Foundation): 国家自然科学基金(51804231);; 湖北省自然科学基金(2018CFB300)
作者(Author): 王雪婷,程朝阳,刘静,卢海龙,贾涓,宋新莉
DOI: 10.13289/j.issn.1009-6264.2020-0052
参考文献(References):
- [1] Ouyang G,Chen X,Liang Y,et al.Review of Fe-6.5 wt%Si high silicon steel—A promising soft magnetic material for sub-kHz application[J].Journal of Magnetism and Magnetic Materials,2019,481:234-250.
- [2] Takada Y,Abe M,Masuda S,et al.Commercial scale production of Fe-6.5 wt.%Si sheet and its magnetic properties[J].Journal of Applied Physics,1988,64(10):5367-5369.
- [3] Haiji H,Okada K,Hiratani T,et al.Magnetic properties and workability of 6.5% Si steel sheet[J].Journal of Magnetism and Magnetic Materials,1996,160(7):109-114.
- [4] Swann P R,Gr?n?s L,Lehtinen B.The B2 and D03 ordering reactions in iron-silicon alloys in the vicinity of the curie temperature[J].Metal Science,1975,9(1):90-96.
- [5] Wittig J E,Frommeyer G.Deformation and fracture behavior of rapidly solidified and annealed iron-silicon alloys[J].Metallurgical and Materials Transactions A,2008,39(2):252-265.
- [6] 毛卫民,杨平.铁基有序合金的结构转变对塑性行为的影响[J].中国科学:技术科学,2012,42(10):1222-1227.MAO Wei-min,YANG Ping.Influence of structure transition on plastic behaviors of iron based ordered alloys[J].Science China:Technology Science,2012,42(10):1222-1227.
- [7] 林均品,叶丰,陈国良,等.6.5 wt%Si高硅钢冷轧薄板制备工艺、结构和性能[J].前沿科学,2007(2):14-27.LIN Jun-pin,YE Feng,CHEN Guo-liang,et al.Fabrication technology,microstructure and properties of Fe-6.5 wt%Si alloy sheets by cold rolling[J].Frontier Science,2007(2):14-27.
- [8] Kim K N,Pan L M,Lin J P,et al.The effect of boron content on the processing for Fe-6.5 wt%Si electrical steel sheets[J].Journal of Magnetism and Magnetic Materials,2004,277(3):331-336.
- [9] Bolfarini C,Silva M C A,Jorge A M,et al.Magnetic properties of spray-formed Fe-6.5%Si and Fe-6.5%Si-1.0%Al after rolling and heat treatment[J].Journal of Magnetism and Magnetic Materials,2008,320(20):653-656.
- [10] Turtelli R S,Penton-Madrigal A,Barbatti C F,et al.Effect of the addition of Cr,Ta and Nb on structural and magnetic properties of Fe-Si alloys[J].Journal of Magnetism and Magnetic Materials,2005,294(2):151-154.
- [11] Li H Z,Liu H T,Liu Z Y,et al.Microstructure,texture evolution and magnetic properties of strip-casting non-oriented 6.5 wt% Si electrical steel doped with cerium[J].Materials Characterization,2015,103:101-106.
- [12] 杨琨,梁永峰,叶丰,等.Nb微合金化Fe14Si2高硅钢冷轧板织构演变规律[J].金属学报,2013,49(11):1411-1415.YANG Kun,LIANG Yong-feng,YE Feng,et al.Texture evolution of Nb micro-alloyed Fe14Si2 high silicon steel during warm rolling[J].Acta Metallurgica Sinica,2013,49(11):1411-1415.
- [13] 程朝阳,刘静,陈文思,等.温轧工艺制备的Fe-6.5 wt%Si-0.5 wt%Cu合金薄板的结构与性能[J].功能材料,2014,45(10):10119-10122.CHENG Zhao-yang,LIU Jing,CHEN Wen-si,et al.The structure and property of the Fe-6.5 wt%Si-0.5 wt%Cu alloy sheet prepared by warm rolling[J].Functional Materials,2014,45(10):10119-10122.
- [14] Wang X L,Li H Z,Liu Z Y,et al.Effect of cooling rate on bending behavior of 6.5 wt.% Si electrical steel thin sheets fabricated by strip casting and rolling[J].Materials Characterization,2016,111:67-74.
- [15] 李志超,孙强,米振莉,等.冷却速度对 1.35% Si 无取向硅钢热轧退火织构的影响[J].材料热处理学报,2016,37(2):104-109.LI Zhi-chao,SUN Qiang,MI Zhen-li,et al.Effect of cooling rate on annealing textures in hot rolled 1.35%Si non-oriented electrical steel[J].Transaction of Materials and Heat Treatment,2016,37(2):104-109.
- [16] Jung H,Kim J.Influence of cooling rate on iron loss behavior in 6.5 wt% grain-oriented silicon steel[J].Journal of Magnetism and Magnetic Materials,2014,353(3):76-81.
- [17] Jung H,Na M,Kim S B,et al.Effect of D03 ordered phase on total loss of 6.5 wt% grain-oriented silicon steel[J].IEEE Transactions on Magnetics,2012,48(11):2921-2924.
- [18] Cheng Z Y,Liu J,Chen W S,et al.Effect of 0.5 mass% Cu addition on ductility and magnetic properties of Fe-6.5Si alloy[J].Journal of Iron and Steel Research International,2016,23(7):717-721.
- [19] Chang S K,Huang W Y.Texture effect on magnetic properties by alloying specific elements in non-grain oriented silicon steels[J].ISIJ International,2005,45(6):918-922.
- [20] 吴圣杰,李慧,岳重祥,等.终轧温度对中低牌号无取向硅钢磁性能的影响[J].材料热处理学报,2019,40(9):89-94.WU Sheng-jie,LI Hui,YUE Chong-xiang,et al.Effect of finishing temperature on magnetic properties of medium and low grade non-oriented silicon steel[J].Transaction of Materials and Heat Treatment,2019,40(9):89-94.
- [21] Qin J,Yang P,Mao W M,et al.Effect of texture and grain size on the magnetic flux density and core loss of cold-rolled high silicon steel sheets[J].Journal of Magnetism and Magnetic Materials,2015,393:537-543.
- [22] 何忠治,赵宇,罗海文.电工钢[M].北京:冶金工业出版社,2012.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||