薄带连铸0.7%Si无取向硅钢的显微组织及织构Microstructure and texture of strip-cast 0. 7% Si non-oriented silicon steel
马良,薛艳春,赵烁,闫涛,岳尔斌,仇圣桃
摘要(Abstract):
采用光学显微镜及电子背散射衍射(EBSD)技术研究了薄带连铸0.7%Si无取向硅钢。结果表明,铸带的显微组织为等轴晶,铸带表层主体织构为{223}<110>,s=0.5层主体织构为{110}<112>和{112}<132>,中心层主体织构为{001}<100>。冷轧板织构主要由较强的<110>//RD和较弱的<111>//ND织构组成。冷轧板经900℃退火后再结晶织构主要由{001}<100>,高斯织构和<111>//ND织构组成,新的立方晶粒易于在剪切带处形核,并在再结晶开始阶段长大成为退火后的主体织构。
关键词(KeyWords): 薄带连铸;织构;储能;无取向;硅钢
基金项目(Foundation): 河北省自然科学基金(E2015402094)
作者(Author): 马良,薛艳春,赵烁,闫涛,岳尔斌,仇圣桃
DOI: 10.13289/j.issn.1009-6264.2015.12.021
参考文献(References):
- [1]马良,项利,仇圣桃,等.正火对双辊薄带连铸5.28%Si-1.11%Al无取向高硅钢磁性能的影响[J].金属热处理,2013,38(6):58-61.MA Liang,XIANG Li,QIU Sheng-tao,et al.Effect of normalizing on magnetic property of5.28%Si-1.11%Al non-orientedhigh silicon steel produced by twin roll thin strip casting[J].Heat Treatment of Metals,2013,38(6):58-61.
- [2]Espedal A B,Roder R.Prospects of thin gauge high-speed strip casting technology[C]//123th TMS Annual Meeting,Lighe Metals,U,Mannweiler,1994:1197-1203.
- [3]Yang M,Pan F.Analysis about forming mechanism of equiaxed crystal zone for 1Cr18Ni9Ti stainless steel twin-roll thin strip[J].Journal of Materials Processing Technology,2009,209(4):2203-2211.
- [4]张元祥,许云波,刘振宇,等.双辊薄带连铸对无取向硅钢织构和磁性能的影响[J].材料热处理学报,2012,33(8):64-68.ZHANG Yuan-xiang,XU Yun-bo,LIU Zhen-yu,et al.Effect of initial grains of twin-roll casting strip on texture andmagnetic properties of a nonoriented electrical steel[J].Transcations of Materials and Heat Treatment,2012,33(8):64-68.
- [5]Zapuskalov N.Comparison of continuous strip casting with conventional technology[J].ISIJ International,2003,43(8):1115-1127.
- [6]Liu H,Liu Z,Li C,et al.Solidification structure and crystallographic texture of strip casting 3wt.%Si non-oriented silicon steel[J].Materials Characterization,2011,62(5):463-468.
- [7]Landgraf F J G,Yonamine T,Takanohashi R,et al.Magnetic properties of silicon steel with as-cast columnar structure[J].Journal of Magnetism and Magnetic Materials,2003,254(1):364-366.
- [8]Zhang Y,Xu Y,Liu H,et al.Microstructure,texture and magnetic properties of strip-cast 1.3%Si non-oriented electrical steels[J].Journal of Magnetism and Magnetic Materials,2012,324(20):3328-3333.
- [9]Kim K N,Pan L M,Lin J P,et al.The effect of boron content on the processing for Fe-6.5 wt%Si electrical steel sheets[J].Journal of Magnetism and Magnetic Materials,2004,277(3):331-336.
- [10]Park J Y,Oh K H,Ra H Y.The Effects of superheating on texture and microstructure of Fe-4.5 wt%Si steel strip by twin-roll strip casting[J].ISIJ International,2001,41(1):70-75.
- [11]Park J T,Szpunar J A.Effect of initial grain size on texture evolution and magnetic properties in nonoriented electrical steels[J].Journal of Magnetism and Magnetic Materials,2009,321(13):1928-1932.
- [12]Li H Z,Liu H T,Liu Z Y,et al.Characterization of microstructure,texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel[J].Materials Characterization,2014,88(2):1-6.
- [13]Xu Y B,Zhang Y X,Wang Y,et al.Evolution of cube texture in strip-cast non-oriented silicon steels[J].Scripta Materialia,2014,87(15):17-20.
- [14]Liu J L,Sha Y H,Zhang F,et al.Development of{210}<001>recrystallization texture in Fe-6.5 wt.%Si thin sheets[J].Scripta Materialia,2011,65(4):292-295.
- [15]Park J T,Szpunar J A.Evolution of recrystallization texture in nonoriented electrical steels[J].Acta Materialia,2003,51(11):3037-3051.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||