微弹性微观相场研究不同时效过程下L12和D022的原子占位(英文)Impact of ageing processes on occupancy probability of L12 and D022 phase:Studied by microelasticity phase field model
张静,陈铮,杨坤,卢艳丽,王永欣
摘要(Abstract):
用包含弹性应变能的微观相场法研究L12-Ni3Al相和D022-Ni3V相在1000K,1200K单温度时效及1000K和1200K交变温度下时效的原子占位。研究表明:从1000K单温度时效经由交变温度时效至1200K单温度时效过程中,L12相中的正位原子NiNi和AlAl及D022相中的正位原子NiNi和Vv的占位几率随时间延长而下降,两种结构中的反位缺陷NiAl,NiV,VNi和AlNi及替代缺陷AlNi,AlV和VNi的占位几率却随时间延长而上升。平衡时的L12相中的NiNi占位几率大于D022相中的NiNi,L12相中的AlAl占位几率小于D022相中的VV,反位缺陷和替代原子在L12相中的占位几率均大于D022相。在交变时效下,原子占位几率的时间演化曲线呈"长城"状,曲线顶点的占位几率值小于相应的单温度时效下的平衡值,但是曲线谷值大于相应的单温度时效下的平衡值。
关键词(KeyWords): 原子占位几率;反位缺陷;替代缺陷;微观相场
基金项目(Foundation): National Natural Science Foundations of China(Grant Nos:50875217,10902086)
作者(Author): 张静,陈铮,杨坤,卢艳丽,王永欣
DOI: 10.13289/j.issn.1009-6264.2010.09.004
参考文献(References):
- [1]Mishin Y.Atomistic modeling of theγandγ′phases of the Ni-Al system[J].Acta Mater,2004,52:451-1467.
- [2]Staron P,Kampmann R.Early-stage decomposition kinetics in Ni-Al alloys—I.Small and wide-angle neutron scattering investigation on Ni-13at%Al and cluster dynamic modeling[J].Acta Mater,2000,48:701-712.
- [3]Staron P,Kampmann R.Early-stage decomposition kinetics in Ni-Al alloys—Ⅱ.Small and wide-angle neutron scattering investigation on Ni-13at.%Al and clusterdy namic modeling[J].Acta Mater,2000,48:713-720.
- [4]Yu S,Wang C Y,Yu T,et al.Self-diffusion in the intermetallic compounds NiAl and Ni3Al:An embedded atom method study[J].Physica B,2007,396:138-144.
- [5]Chen G X,Wang D D,Zhang J M,et al.Self-diffusion of Ni in the intermetallic compound Ni3Al[J].Physica B,2008,403:3538-3542.
- [6]Jiri Cermak,Ales Gazda,Vera Rothova.Interdiffusion in ternary Ni3Al/Ni3Al-X diffusion couples with X=Cr,Fe,Nb and Ti[J].Intermetallics,2003,11:939-946.
- [7]Geng C Y,Wang CY,Yu T.Site preference and alloying effect of platinum group metals inγ′-Ni3Al[J].Acta Mater,2004,52:5427-5433.
- [8]Sluiter H F M,Kawazoe Y.Site preference of ternary additions in Ni3Al[J].Phys Rev B,1995,51:4062-4073.
- [9]Chen G L,Lin J P.Ordered Intermetallic of Structural Materials[M].Beijing:Metallurgical Industry Press,1999.
- [10]Cabet E,Pasturel A,Ducastelle F,et al.L12-D022Competition in the pseudobinary(Pt,Rh)3V,Pt3(V,Ti),and(Pd,Rh)3V alloys:Phase stability and electronic structure[J].Phys Rev Lett,1996,76:3140-3143.
- [11]Prakash U,Buckley R A,Jones H,et al.D022to L12transition in intermetallic systems[J].J Mater Sci,1992,27:2001-2004.
- [12]Xu J H,Oguchi T,Freeman A J.Solid-solution strengthening:substitution of V in Ni3Al and structural stability of Ni3(Al,V)[J].Phys Rev B,1987,36:4186-4189.
- [13]Zapolsky H,Pareige C,Marteau L,et al.Atom probe analyses and numerical calculation of ternary phase diagram in Ni-Al-V system[J].Calphad,2001,25:125-134.
- [14]Prakash U,Buckley R A,Jones H,et al.D022to L12transition in intermetallic systems[J].J Mater Sci,1992,27:2001-2004.
- [15]Mekhrabov A O,Akdeniz M V,A Arer M M.Atomic ordering characteristics of Ni3Al intermetallics with substitutional ternary additions[J].Acta Mater,1997,45:1077-1083.
- [16]Sluiter Marcel H F,Kawazoe Y.Site preference of ternary additions in Ni3Al[J].Phys Rev B,1995,51(7):4062-4073.
- [17]Ruban A V,Skriver H L.Calculated site substitution in ternaryγ′-Ni3Al:Temperature and composition effects[J].Phys Rev B,1997,55(2):856-874.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||