球磨法制备Sn-Co合金及其可逆储锂性能Synthesis and lithium storage performance of Sn-Co alloy prepared by ball milling method
沈丁,杨绍斌,张淑凯,薛维华
摘要(Abstract):
以原子比为1∶1的Co与Sn金属粉为原料,采用球磨法制备了锂离子电池负极Sn-Co合金,研究了其形成机理及可逆储锂性能。结果表明,球磨先形成CoSn3和CoSn2等中间相,最后形成CoSn2相,继续球磨,CoSn2相的晶粒尺寸先逐渐减小后趋于稳定。晶粒的细化有利于提高合金的首次可逆容量和循环性能,球磨50 h后,首次可逆容量接近最大值,为426 mAh/g,30次循环后容量保持率为67.1%。热处理后,物相转变为CoSn相,提高了合金的循环性能,30次循环后容量保持率为73.7%,但热处理过程中晶粒和颗粒的长大使首次可逆容量降低。
关键词(KeyWords): 锂离子电池;Sn-Co;球磨;热处理;电化学性能
基金项目(Foundation): 辽宁省自然科学基金(20072206)
作者(Author): 沈丁,杨绍斌,张淑凯,薛维华
DOI: 10.13289/j.issn.1009-6264.2010.12.029
参考文献(References):
- [1]沈丁,杨绍斌,张淑凯.锂离子电池锡钴和锡钴碳负极材料的研究进展[J].化工进展,2008,27(12):1892-1896.SHEN Ding,YANG Shao-bin,ZHANG Sui-kai.Development of Sn-Co and Sn-Co-C anode materials for Li-ion batteries[J].Chem Ind Eng Prog,2008,27(12):1892-1896.
- [2]何见超,赵海雷,贾喜娣,等.锂离子电池Sn-Co合金负极材料的研究进展[J].化工学报,2009,60(5):1073-1079.HE Jian-chao,ZHAO Hai-lei,JIA Xi-di.et al.Research progress of Sn-Co anode materials for lithium-ion batteries[J].CIESC Journal,2009,60(5):1073-1079.
- [3]Todd A D W,Mar R E,Dahn J R.Combinatorial study of tin-transition metal alloys as negative electrodes for lithium-ion batteries[J].JElectrochem Soc A,2006,153(10):1998-2005.
- [4]Dahn J R,Mar R E,Abouzeid Alyaa.Combinatorial study of Sn1-x Cox(0
- [5]Tamura N,Fujimoto M,Kamino M,et al.Mechanical stability of Sn-Co alloy anodes for lithium secondary batteries[J].Electrochimica Acta,2004,49(12):1949-1956.
- [6]张敬君,夏永姚.锂离子电池负极材料Sn-Co合金的研究进展[J].高等学校化学学报,2006,27(10):1923-1926.ZHANG Jin-jun,XIA Yong-yao.CoSn Alloys as negative electrode materials for lithium-ion batteries[J].Chem J Chin Univ,2006,27(10):1923-1926.
- [7]沈丁.过渡元素对Sn-Co/C基负极材料的结构和电性能的影响[D].阜新:辽宁工程技术大学,2009:23-31.SHEN Ding.Influence of transition element on structure and electrochemcial performance of Sn-Co/C based anoode material[D].Fuxin:LiaoningTechnical University,2009:23-31.
- [8]任榕,吴玉程,汤文明,等.退火诱导机械合金化Fe42.5Al42.5Ti5B10合金的结构演变与晶粒生长动力学[J].物理学报,2008,57(9):5774-5781.REN Rong,WU Yu-cheng,TANG Wen-ming,et al.Structural evolution and grain growth kinetics of the mechanically alloyed Fe42.5 Al42.5 Ti5 B10induced by annealing[J].Acta Physica Sinica,2008,57(9):5774-5781.
- [9]Yang J,Takeda Y,Imanishi N,et al.Ultrafine Sn and SnSb0.14 powders for lithium storage matrices in lithium-Ion batteries[J].J Electrochem Soc,1999,146(11):4009-4013.
- [10]张宁,于维平.电沉积制备锡钴碳复合负极材料的结构与性能[J].材料热处理学报,2008,29(6):5-8,13.ZHANG Ning,YU Wei-ping.Structure and performance of Sn-Co-C composite negative material prepared by electrodepositing[J].Trans Mater HeatTreat,2008,29(6):5-8,13.
- [11]杨绍斌,沈丁,李强.Sn0.35-0.5xCo0.35-0.5xZnxC0.3复合材料的制备及电化学性能[J].金属学报,2010,46(1):6-12.YANG Shao-bin,SHEN Ding,LI Qiang.Synthesis and electrochemical properties of Sn0.35-0.5xCo0.35-0.5xZnxC0.3 composite[J].Acta MetallurgicaSinica,2010,46(1):6-12.
- [12]王忠,田文怀,李星国.Sn-Sb合金的氢电弧等离子体法制备及其电化学性能[J].物理化学学报,2006,22(6):752-755.WANG Zhong,TIAN Wen-huai,LI Xing-guo.Synthesis and electrochemical properties of Sn-Sb alloy prepared by hydrogen plasma-metal reaction[J].Acta Phys-Chim Sin,2006,22(6):752-755.
- [13]Zhang J J,Xia Y Y.Co-Sn alloys as negative electrode materials for rechargeable lithium batteries[J].J Electrochem Soc A,2006,153(8):1466-1471.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||