WE43镁合金半固态坯料的制备及其组织演变分析Preparation of semi-solid billet of WE43 magnesium alloy and its microstructure evolution analysis
段兴旺,谈芸芸,辛向前,车鑫,江冬
摘要(Abstract):
采用应变诱发熔化激活法(SIMA)制备WE43镁合金半固态坯料,研究保温温度和保温时间对其半固态组织的影响,分析了不同工艺参数下合金的平均晶粒尺寸、液相率及固相形状因子的变化规律,探讨半固态组织演变机制。结果表明:随着保温温度升高和保温时间延长,WE43镁合金的平均晶粒尺寸和液相率显著增加,而固相形状因子则呈现先上升后下降的趋势;半固态组织由α-Mg晶粒、晶界液相及晶内“小液池”组成,其晶粒演变过程分为初始长大、球化分离及合并粗化3个阶段,演变机制为Ostwald熟化机制和晶粒合并长大机制;采用SIMA工艺制备WE43镁合金半固态坯料的最佳工艺为在610℃保温45 min。
关键词(KeyWords): WE43镁合金;SIMA;半固态坯料;组织演变
基金项目(Foundation): 山西省基础研究计划资助项目(202203021211191)
作者(Author): 段兴旺,谈芸芸,辛向前,车鑫,江冬
DOI: 10.13289/j.issn.1009-6264.2025-0097
参考文献(References):
- [1] Chen Q,Shu D,Zhao Z D,et al.Microstructure development and tensile mechanical properties of Mg-Zn-RE-Zr magnesium alloy[J].Materials & Design,2012,40:488-496.
- [2] Chen Q,Shu D Hu C,et al.Grain refinement in an as-cast AZ61 magnesium alloy processed by multi-axial forging under the multitemperature processing procedure[J].Materials Science and Engineering A,2012,541:98-104.
- [3] Luo A A.Magnesium casting technology for structural applications[J].Journal of Magnesium and Alloys,2013,1(1):2-22.
- [4] Markini V,Pai P S,Bolar G,et al.Cryogenic and conventional milling of AZ91 magnesium alloy[J].Journal of Magnesium and Alloys,2024,12(6):2503-2519.
- [5] Chang Z,Deng Q,Wu Y,et al.Semi-solid rheo-diecast Mg-xGd-3Y-1Zn-0.4Zr (wt%) alloys and their comparison with conventional HPDC alloys[J].Journal of Alloys and Compounds,2024,1003:175508.
- [6] Zhou K,Lu Q H,Qin J N,et al.A view of magnesium alloy modification and its application in orthopedic implants[J].Journal of Materials Research and Technology,2025,36:1536-1561.
- [7] 段兴旺,贾悦,陈迎庆,等.WE43镁合金的均质化处理及本构模型建立[J].金属热处理,2024,49(10):185-190.DUAN Xing-wang,JIA Yue,CHENG Ying-qing,et al.Homogenization treatment and establishment of constitutive model for WE43 magnesium alloy[J].Heat Treatment of Metals,2024,49(10):185-190.
- [8] Luo T J,Yang Y S,Li Y J,et al.Influence of rare earth Y on the corrosion behavior of as-cast AZ91 alloy[J].Electrochimica Acta,2009,54(26):6433-6437.
- [9] Brar H S,Berglund I S,Allen J B,et al.The role of surface oxidation on the degradation behavior of biodegradable Mg-RE (Gd,Y,Sc) alloys for resorbable implants[J].Materials Science and Engineering C,2014,40:407-417.
- [10] Guo X,Zhao H,Song J,et al.Effect of Ca on hot tearing susceptibility of WE43 alloy[J].Journal of Alloys and Compounds,2024,1002:175451.
- [11] Yang L,Huang Y,Hou Z,et al.Microstructure,mechanical properties and fracture behaviors of large-scale sand-cast Mg-3Y-2Gd-1Nd-0.4Zr alloy[J].Journal of Magnesium and Alloys,2023,11(8):2763-2775.
- [12] Thanabal N,Silambarasan R,Seenuvasperumal P,et al.Microstructure and mechanical behavior of AXM Mg alloy systems:A review[J].Journal of Magnesium and Alloys,2024,12(7):2624-2646.
- [13] Chen X,Zhang J,Wang M,et al.Research progress of heterogeneous structure magnesium alloys:A review[J].Journal of Magnesium and Alloys,2024,12(6):2147-2181.
- [14] Bhattacharyya J J,Agnew S R,Muralldharan G.Texture enhancement during grain growth of magnesium alloy AZ31B[J].Acta Materialia,2015,86:80-94.
- [15] Fleming M C.Behavior of metal alloys in the semisolid state[J].Metallurgical Transactions B,1991,22:269-293.
- [16] Pola A,Tocci M,Kapranos P.Microstructure and properties of semi-solid aluminum alloys:A literature review[J].Metals-Open Access Metallurgy Journal,2018,8(3):181-186.
- [17] Chen Q,Zhao Z,Zhao Z,et al.Microstructure development and thixoextrusion of magnesium alloy prepared by repetitive upsetting-extrusion[J].Journal of Alloys and Compounds,2011,509(26):7303-7315.
- [18] Fu J L,Jiang H J,Wang K K,et al.influence of processing parameters on microstructural evolution and tensile properties for 7075 Al alloy prepared by an ECAP-based SIMA process[J].Acta Metallurgica Sinica (English Letters),2018,31(4):337-350.
- [19] 王佳,肖寒,吴龙彪,等.轧制-重熔SIMA法制备ZCuSn10合金半固态坯料[J].金属学报,2014,50(5):567-574.WANG Jia,XIAO Han,WU Long-biao,et al.Study of rolling-remelting SIMA process for preparing the semi-solid billet of ZCuSn10 alloy[J].Acta Metallurgica Sinica,2014,50(5):567-574.
- [20] Wang X,Sun K,Wang C,et al.Influence of solute content and cooling rate on the preparation of semi-solid slurries for novel creep-resistant Mg-Gd-Ca-Zr alloys[J].Journal of Materials Research and Technology,2024,31:1409-1418.
- [21] Lou W,Li X,Wei S,et al.Effect of Y2O3 on high temperature thermal compression performance of Cu-10W composites and microstructure analysis[J].Ceramics International,2024,50(21):43586-43603.
- [22] Dong Y H,Zhang D,Li D G,et al.Control of Ostwald ripening[J].Science China (Materials),2023,66(3):1249-1255.
- [23] Li G,Qu W Y,Luo M,et al.Semi-solid processing of aluminum and magnesium alloys:Status,opportunity,and challenge in China[J].Transactions of Nonferrous Metals Society of China,2021,31(11):3255-3280.
- [24] Li H,Cao M,Niu L,et al.Establishment of macro-micro constitutive model and deformation mechanism of semi-solid Al6061[J].Journal of Alloys and Compounds,2021,854:157124.
- [25] Kleiner S,Beffort O,Uggowitzer P J.Microstructure evolution during reheating of an extruded Mg-Al-Zn alloy into the semisolid state[J].Scripta Materialia,2004,51(5):405-410.
- [26] Atkinson H V,Liu D.Microstructural coarsening of semi-solid aluminium alloys[J].Materials Science and Engineering A,2008,496(1):439-446.
- [27] 李淑颖,杨书环.研究型物理化学综合实验教学探究-利用扫描隧道显微镜原位观察表面奥斯特瓦尔德熟化现象[J].广东化工,2024,51(21):227-228.LI Shu-ying,YANG Shu-huan.Exploring the comprehensive experimental teaching of research-based physical chemistry:In-situ observe interfacial Ostwald ripening phenomena using a scanning tunneling microscope[J].Guangdong Chemical Industry,2024,51(21):227-228.
- [28] 曹苗,赵娟娟,张琦.SIMA法制备半固态材料过程中球状晶粒粗化机制的研究[J].精密成形工程,2020,12(6):37-43.CAO Miao,ZHAO Juan-juan,ZHANG Qi.Mechanism of spherical grain coarsening in preparation of semi-solid materials by SIMA method[J].Journal of Netshape Forming Engineering,2020,12(6):37-43.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||