新型含氮奥氏体热作模具钢的研究Research on a new nitrogen-bearing austenitic hot work die steel
江浩,吴晓春
摘要(Abstract):
对一种新型含氮奥氏体模具钢在不同工艺下进行热处理,并对试验钢的强韧性与热稳定性进行测试。利用DIL805A热膨胀相变仪测定膨胀系数,通过光学显微镜、高分辨扫描电子显微镜、X射线衍射仪及高分辨透射电子显微镜观察分析显微组织。结果表明:试验钢的最佳热处理工艺为1200℃固溶+720℃时效保温2 h,硬度达46 HRC,横向无缺口冲击试样冲击功达150 J;热稳定性良好,700℃保温20 h,硬度基本不变,780℃保温20 h后,硬度在44 HRC以上;钢中析出相主要为V(C、N),时效状态下析出相占钢中总量约4%,弥散析出强化相尺寸为10~20 nm。
关键词(KeyWords): 含氮奥氏体钢;热稳定性;析出相
基金项目(Foundation): 国家“十一五”科技支撑计划课题(2007BAE51B04);; 上海市重点学科建设项目(S30107)
作者(Author): 江浩,吴晓春
DOI: 10.13289/j.issn.1009-6264.2011.03.015
参考文献(References):
- [1]朱宗元.我国热作模具钢性能数据集(续Ⅶ)[J].机械工程材料,2001,25(8):38-42.ZHU Zong-yuan.Property data collection of common hot working die steels used in China[J].Materials for Mechanical Engineering,2001,25(8):38-42.
- [2]崔崑.国内外模具用钢发展概况[J].金属热处理,2007,32(1):1-11.CUI Kun.Development of die and mould steels at home and abroad[J].Heat Treatment of Metals,2007,32(1):1-11.
- [3]黄春峰.国外新型热作模具钢及其热处理工艺[J].航空制造技术,2003(8):68-70.HUANG Chun-feng.New type of hot-mold steel and its heat treatment process abroad[J].Aeronautical Manufacturing Technology,2003(8):68-70.
- [4]Kamachi Mudali U,Baldev Raj.High Nitrogen Steels and Stainless Steels—Manufacturing,Properties and Applications[M].Narosa PublishingHouse,2006:2-4,5-7,48-63,141.
- [5]Simmons J W.Overview:high-nitrogen alloying of stainless steels[J].Materials Science and Engineering,1996,207(2):159-169.
- [6]逯允海,付瑞东,邱亮,等.氮强化高锰奥氏体钢热变形行为研究[J].材料热处理学报,2007,28(2):69-72.LU Yun-hai,FU Rui-dong,QIU Liang,et al.Deformation behavior of nitrogen strengthened high manganese austenitic steel[J].Transactions ofMaterials and Heat Treatment,2007,28(2):69-72.
- [7]沈国雄,刘斌.氮对304奥氏体不锈钢组织和力学性能的影响[J].钢铁研究学报,1997,9(6):33-36.SHEN Guo-xiong,LIU Bin.Effect of nitrogen on structure and mechanical properties of 304 austenitic stainless steel[J].Journal of Iron and SteelResearch,1997,9(6):33-36.
- [8]Jack D H,Jack K H.Invited review:Carbides and nitrides in steel[J].Materials Science and Engineering,1973,11(1):1-27.
- [9]王良平,吴晓春.影响奥氏体热作模具钢性能的因素[J].钢铁,2008,43(11):78-81.WANG Liang-ping,WU Xiao-chun.Influencing factors of performance for austenitic hot die work steel[J].Iron and Steel,2008,43(11):78-81.
- [10]屠怡范,张建福,赵栋梁,等.Fe-Ni基高强度低膨胀合金组织性能与时效时间的关系[J].金属功能材料,2007,14(3):10-14.TU Yi-fan,ZHANG Jian-fu,ZHAO Dong-liang,et al.Relations between aging treatment time and microstructure and properties of Fe-Ni based highstrength low thermal expansion alloy[J].Metallic Functional Materials,2007,14(3):10-14.
- [11]陆建生,毛彭龄,倪和勇,等.Fe-38Ni-Mo-V-C低膨胀合金碳化物析出规律的研究[J].宝钢技术,2005,5:30-33.LU Jian-sheng,MAO Peng-ling,NI He-yong,et al.Research on precipitation law on carbide of low expansion alloy Fe-38Ni-Mo-V-C[J].BaoSteel Technology,2005,5:30-33.
- [12]谢长生,何向山,崔崑.奥氏体热作工具钢的晶粒粗化行为及合金元素的作用[J].金属学报,1986,22(6):A461-A469.XIE Chang-sheng,HE Xiang-shan,CUI Kun.Grain coarsening behaviour towards austenitic hot work tool steels and effect of alloying elements[J].Acta Metallurgica Sinica,1986,22(6):A461-A469.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||