Super304H奥氏体耐热钢服役36891 h后的组织与性能Microstructure and properties of Super304H austenitic heat-resistant steel after service for 36891 h
王伟,黄翔,蔡永江,李文胜,高岩
摘要(Abstract):
利用光学显微镜、扫描电子显微镜、能谱分析仪、X-射线衍射仪、拉伸试验机和电化学工作站等研究了服役36891 h的Super304H过热器管的组织及性能变化。结果表明,服役36891 h管的强度仍满足GB/T 5310-2008的规定,伸长率略低于标准。服役管基体组织为奥氏体和孪晶组织,晶粒粗大,晶界大量析出呈链状分布M23C6。经DL-EPR分析,服役36891 h管的晶间腐蚀敏感性较供货态新管显著升高。
关键词(KeyWords): Super304H;高温运行;组织;力学性能;晶间腐蚀敏感性
基金项目(Foundation): 南方电网公司科技项目(K-GD2014-162);; 国家自然科学基金(51471072)
作者(Author): 王伟,黄翔,蔡永江,李文胜,高岩
DOI: 10.13289/j.issn.1009-6264.2015.10.015
参考文献(References):
- [1]迟成宇,董建新,刘文庆,等.3DAP研究Super304H耐热不锈钢中富Cu相的析出行为[J].金属学报,2010,46(9):1141-1146.CHI Cheng-yu,DONG Jian-xin,LIU Wen-qing,et al.3DAP investigation of precipitation behavior of Cu-rich phase in Super304H heat resistant steel[J].Acta Metallugica Sinica,2010,46(9):1141-1146.
- [2]Isheim D,Vaynman S,Fine M E,et al.Copper-precipitation hardening in a non-ferromagnetic face-centered cubic austenitic steel[J].Scripta Materialia,2008,59(12):1235-1238.
- [3]Sawaragi Y,Otsuka N,Senba H,et al.Properties of a new 18-8 austenitic steel tube(SUPER 304H)for fossil fired boilers after service exposure with high elevated temperature strength[J].The Sumitomo Search,1994(56):34-43.
- [4]GAO Yan,ZHANG Chun-lei,XIONG Xia-hua.Intergranular corrosion susceptibility of a novel Super304H stainless steel[J].Engineering Failure Analysis,2012,24(9):26-32.
- [5]王剑志,罗仕清,黄晓斌.超(超)临界锅炉用Super304H钢管研究试制[J].钢铁,2006,41(1):43-46.WANG Jian-zhi,LUO Shi-qing,HUANG Xiao-bin.Trial production of Super304H tubes for supercritical(ultra-super critical)boiler[J].Iron and Steel,2006,41(1):43-46.
- [6]刘正东,程世长,杨钢,等.中国超超临界火电机组用S30432钢管研制[J].钢铁,2010,45(6):1-6.LIU Zheng-dong,CHENG Shi-chang,YANG Gang,el at.Research and development of S30432 steel tubes in China used for ultra supercritical(USC)power plants[J].Iron and Steel,2010,45(6):1-6.
- [7]李新梅.Super304H奥氏体钢焊接接头组织与性能研究[D].山东大学博士学位论文,2010.
- [8]Li X M,Zou Y,Zhang Z W,el at.Intergranular corrosion of weld meld of Super Type 304H steel during 650℃aging[J].Corrosion,2012,68(5):379-387.
- [9]张春雷,熊夏华,郑志军,等,稳定化处理对Super304H奥氏体耐热钢晶间腐蚀敏感性的影响[J].材料研究学报,2013,27(4):411-418.ZHANG Chun-lei,XIONG Xia-hua,ZHENG Zhi-jun,et al.Influence of Stabilization Treatment on the Intergranular Corrosion Susceptibility of Super304H Austenitic Heat-resistant Steel[J].Chinese Journal of Materials Research,2013,27(4):411-418.
- [10]ZHANG Chun-lei,XIONG Xia-hua,PING Shao-bo,et al,Influence of chemical composition on the intergranular corrosion susceptibility of Super304H austenitic heat-resistant steel[J].Corrosion Engineering Science and Technology,2014,49(7):624-632.
- [11]熊夏华.新型锅炉耐热不锈钢Super304H的抗晶间腐蚀性能研究[D].华南理工大学硕士学位论文,2012.
- [12]赵林,董显平,孙锋,等.Super304H超超临界锅炉过热器管长期服役后的显微组织及力学性能[J].机械工程材料,2013,37(7):28-32.ZHAO Lin,DONG Xian-ping,SUN Feng,el at.Microstructure and mechanical properties of Super304H ultra supercritical pressure boiler superheater tube after serving for a long time[J].Materials for Mechanical Engineering,2013,37(7):28-32.
- [13]Peltonen M,Lindroos T,Kallio M.Effect of ageing on transformation kinetics and internal friction of Ni-rich Ni-Ti alloys[J].Journal of Alloys and Compounds,2008,460(1):237-245.
- [14]Beltran R,Maldonado J G,Murr L E,et al.Effects of strain and grain size on carbide precipitation and corrosion sensitization behavior in 304 stainless steel[J].Acta Materialia,1997,45(10):4351-4360.
- [15]Sahlaoui H,Makhlouf K,Sidhom H,et al.Effects of ageing conditions on the precipitates evolution,chromium depletion and intergranular corrosion susceptibility of AISI 316L:experimental and modeling results[J].Materials Science and Engineering A,2004,372(1):98-108.
- [16]Taiwade R V,Shukla R,Vashishtha H,et al.Effect of grain size on degree of sensitization of chrome-manganese stainless steel[J].ISIJ International,2013,53(12):2206-2212.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||