较短临界退火时间下中锰TRIP钢的组织及力学性能Microstructure and mechanical properties of a medium Mn TRIP steel under short intercritical annealing time
定巍,杜敬超,李岩,龚志华,潘红波
摘要(Abstract):
利用拉伸试验机、扫描电镜、透射电镜以及X射线衍射分析了临界退火温度和临界退火时间对中锰钢的微观组织以及力学性能的影响。研究结果表明:在本文所设计工艺条件下,由于临界退火时间短导致组织中的渗碳体无法完全溶解,其微观组织主要由铁素体、残留奥氏体以及渗碳体所构成;试样在650~700℃之间退火能获得良好性能,但是不同临界退火温度出现良好力学性能所需要的时间不一样,温度越高,所需要时间越短;675℃退火5 min时有最佳的力学性能,抗拉强度约为980 MPa,断后伸长率约为30%,强塑积接近30 GPa·%。
关键词(KeyWords): 连续退火;中锰TRIP钢;微观组织;力学性能
基金项目(Foundation): 国家自然科学基金(51304120,51364033);; 内蒙古自然科学基金(2015MS0556,2015MS0557)
作者(Author): 定巍,杜敬超,李岩,龚志华,潘红波
DOI: 10.13289/j.issn.1009-6264.2017.04.017
参考文献(References):
- [1]Lee Y K,Han J.Current opinion in medium manganese steel[J].Materials Science and Technology,2015,31(7):843-856.
- [2]董瀚,王毛球,翁宇庆.高性能钢的M3组织调控理论与技术[J].钢铁,2010,45(7):1-6.DONG Han,WANG Mao-qiu,WENG Yu-qing.Performance improvement of steels through M3structure control[J].Iron and Steel,2010,45(7):1-6.
- [3]Seo C H,Kwon K H,Choi K,et al.Deformation behavior of ferrite-austenite duplex lightweight Fe-Mn-Al-C steel[J].Scripta Materialia,2012,66(8):519-522.
- [4]Edmonds D V,He K,Rizzo F C,et al.Quenching and partitioning martensite-A novel steel heat treatment[J].Materials Science and Engineering A,2006,438-440(24):25-34.
- [5]董瀚,曹文全,时捷,等.第3代汽车钢的组织与性能调控技术[J].钢铁,2011,46(6):1-11.DONG Han,CAO Wen-quan,SHI Jie,et al.Microstructure and performance control technology of the 3rdgeneration auto sheet steels[J].Iron and Steel,2011,46(6):1-11.
- [6]刘永刚,潘红波,詹华,等.几种典型第三代汽车用先进高强度钢技术浅析[J].金属热处理,2015,40(8):13-19.LIU Yong-gang,PAN Hong-bo,ZHAN Hua,et al.Introduction of several typical 3rd generation AHSS for automotive industry[J].Heat Treatment of Metals,2015,40(8):13-19.
- [7]Han J,Lee S Joon,Jung J G,et al.The effects of the initial martensite microstructure on the microstructure and tensile properties of intercritically annealed Fe-9Mn-0.05C steel[J].Acta Materialia,2014,78:369-377.
- [8]Gibbs P J,Moor E De,Merwin M J,et al.Austenite stability effects on tensile behavior of manganese-enriched-austenite transformation-induced plasticity steel[J].Metallurgical and Materials Transactions A,2011,42(12):3691-3702.
- [9]Lee S,Cooman B C De.On the selection of the optimal intercritical annealing temperature for medium Mn TRIP steel[J].Metallurgical and Materials Transactions A,2013,44(11):5018-5024.
- [10]Luo H W,Shi J,Wang C,et al.Experimental and numerical analysis on formation of stable austenite during the intercritical annealing of 5Mn steel[J].Acta Materialia,2011,59(10):4002-4014.
- [11]Zhao C,Zhang C,Cao W Q,et al.Observation on formation of fresh martensite from the reversed austenite during water-quenching process in Fe-0.2C-5Mn steel[J].Metallurgical and Materials Transactions A,2015,46(9):3789-3792.
- [12]Cai Z H,Ding H,Misra R D K,et al.Austenite stability and deformation behavior in a cold-rolled transformation-induced plasticity steel with medium manganese content[J].Acta Materialia,2015,84:229-236.
- [13]赵征志,尹鸿祥,赵爱民,等.连续退火对5%Mn超细晶TRIP钢组织性能的影响[J].材料科学与工艺,2014,22(10):54-59.ZHAO Zheng-zhi,YIN Hong-xiang,ZHAO Ai-min,et al.Effect of continuous annealing process on microstructure and mechanical properties of 5%Mn ultrafine grain TRIP steel[J].Materials Science&Technology,2014,22(10):54-59.
- [14]Xu H F,Zhao J,Cao W Q,et al.Heat treatment effects on the microstructure and mechanical properties of a medium manganese steel(0.2C-5Mn)[J].Materials Science and Engineering A,2012,532(1):435-442.
- [15]Dong W S,Ryu J H,Joo M S,et al.Medium-alloy manganese-rich transformation induced plasticity steels[J].Metallurgical and Materials Transactions A,2013,44(1):286-293.
- [16]Nakada N,Mizutani K,Tsuchiyama T,et al.Difference in transformation behavior between ferrite and austenite formations in medium manganese steel[J].Acta Materialia,2014,65(65):251-258.
- [17]Luo H W,Qiu C H,Dong H,et al.Experimental and numerical analysis of influence of carbide on austenitisation kinetics in 5Mn TRIP steel[J].Materials Science and Technology,2014,30(11):1367-1377.
- [18]定巍,龚志华,唐荻,等.低硅含铝TRIP钢残余奥氏体变形过程中的稳定性研究[J].材料工程,2013(12):68-73.DING Wei,GONG Zhi-hua,TANG Di,et al.Stability of retained austenite of low Si containing Al TRIP steel during deformation[J].Journal of Materials Engineering,2013(12):68-73.
- [19]定巍,杜敬超,龚志华,等.奥氏体化温度对TAM钢力学性能及微观组织影响[J].材料热处理学报,2016,37(8):119-124.DING Wei,DU Jing-chao,GONG Zhi-hua,et al.Influence of austenitizing temperature on mechanical property and microstructure of TAM steel[J].Transactions of Materials and Heat Treatment,2016,37(8):119-124.
- [20]Luo H W,Liu J H,Dong H,A novel observation on cementite formed during intercritical annealing of medium Mn steel[J].Metallurgical and Materials Transactions A,2016,47(6):3119-3124.
- [21]Fei H Y,Jia Y Y,Annika B,et al,Austenite reversion during intercritical annealing in a medium-Mn steel:simulations and experiments[C].TMS2016,145th Annual Meeting and Exhibition,Nashville,Tennessee,USA,2016.