合金元素和工艺参数对非调质CT80钢组织性能影响Effect of alloy elements and process parameters on microstructure and properties of non-quenched and tempered CT80 steel
周乐育,李明扬,刘雅政,袁付春
摘要(Abstract):
研究了终轧温度、冷却速度和卷取温度等工艺参数对具有不同Mo、Nb含量的非调质CT80连续油管用钢组织性能的影响。结果表明,满足其强韧性要求的组织特征为针状铁素体和贝氏体复相组织,且弥散分布约4%的细小M/A岛。终轧温度主要影响组织均匀性。当冷却速度由40~45℃/s提高到60~70℃/s后,铁素体形态转变为针状,其内部亚晶面积增加,位错密度升高。卷取温度影响复相组织中强化相的形态与分布。为避免珠光体或马氏体而促进贝氏体组织转变充分,卷取温度应约为450℃。Mo元素含量提高至0.24%可促进针状铁素体转变并形成细小的强化相M/A岛,起到良好的亚结构强化和相变强化效果。Mo和Nb含量的增加使得实验钢对冷速的敏感性明显降低,增强了非调质CT80连续油管用钢控冷过程工艺稳定性。
关键词(KeyWords): 连续油管用钢;复相组织;冷却速度;卷取温度
基金项目(Foundation): 中央高校基本科研业务费专项资金资助(FRF-TP-12-046A)
作者(Author): 周乐育,李明扬,刘雅政,袁付春
DOI: 10.13289/j.issn.1009-6264.2013.05.017
参考文献(References):
- [1]王少力,郑子元.连续油管国产化技术研究新进展[J].石油矿场机械,2008,37(1):91-93.WANG Shao-li,ZHENG Zi-yuan.New progress in manufacture technology of domestic coiled tubing[J].Oil Field Equipment,2008,37(1):91-93.
- [2]彭在美,陡树柏,董帅,等.连续油管国内外应用现状级国内的研制方向[J],焊管,2008,31(4):7-13.PENG Zai-mei,DOU Shu-bai,DONG Shuai,et al.Coiled tubing application at home and aboard and direction of China coiled tubing research[J].Welded Pipe and Tube,2008,31(4):7-13.
- [3]赵广慧,梁政.连续油管力学性能研究进展[J].钻采工艺,2008,31(4):97-101.ZHAO Guang-hui,LIANG Zheng.Research on mechanical property of coiled tubing[J].Drilling&Production Technology,2008,31(4):97-101.
- [4]陈会年,张国龙,胡清富.连续油管钻井技术的发展及应用[J].石油钻探技术,2000,28(4):19-21.CHEN Hui-nian,ZHANG Guo-long,HU Qing-fu.Developments and applications of coiled tubing drilling techniques[J].Petroleum DrillingTechniques,2000,28(4):19-21.
- [5]Gaddy D E.Coiled tubing drilling technologies target niche markets[J].Oil&Gas Journal,2000,98(2):29-34.
- [6]Behenna F R,Myrick D D,Stanley P K,et al.Field validation of a CT fatigue model[C].SPE 81726-MS,2003.
- [7]Dingley D J,Field D P.Electron backscatter diffraction and orientation imaging microscopy[J].Journal of Materials Science&Technology,1997,13(1):69-78.
- [8]王伟,朱林,胡平,等.针状铁素体管线钢的组织结构及其与力学性能的关系研究[J].焊管,2009,32(11):21-28.WANG Wei,ZHU Lin,HU Ping,et al.Study on microstructures and relation between microstructures and mechanical properties of acicular ferritepipeline steel[J].Welded Pipe and Tube,2009,32(11):21-28.
- [9]刘刚,曲占元.针状铁素体钢的力学性能与显微结构[J].材料开发与应用,2010,25(1):6-8.LIU Gang,QU Zhan-yuan.Mechanical propertie and microstructure for acicular ferrite steel[J].Development and Application of Materials,2010,25(1):6-8.
- [10]廖波,肖福仁.管线用超低碳钢中针状铁素体的形成及强韧化行为[J].材料热处理学报,2009,30(2):57-62.LIAO Bo,XIAO Fu-ren.Research on microstructure and strength-toughening mechanism of acicular ferrite pipeline steel[J].Transactions of Materialsand Heat Treatment,2009,30(2):57-62.
- [11]Pereloma E V,Bayley C,Boyd J D.Microstructural evolution during Simulated OLAC processing of a low-carbon micro alloyed steel[J].MaterialsScience and Engineering A,1996,216:16-24.
- [12]Lee W B,Hong S G,Park C G,et al.Influence of Mo on precipitation hardening in hot rolled HSLA steels containing Nb[J].Scripta Materialia,2000,43(4):319-324.
- [13]Motohashi H,Hagiwara N,Masuda T.Tensile properties and microstructure of weld metal of X80 steel[J].Mater Sci Forum,2003,426:4013-4018.
- [14]Petrov R,Kestens L,Houbaert Y.Characterization of the microstructure and transformation behaviour of strained and nonstrained austenite in Nb-Valloyed C-Mn steel[J].Materials Characterization,2004,53(1):51-61.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||