G115和T92钢表面FeAl渗层制备及其抗高温水蒸汽氧化性能Preparation of FeAl penetration layer on G115 and T92 steel surface and its oxidation resistance to high temperature steam
董猛,谢逍原,朱阳存,杨淑莉,刘光明,汪元奎
摘要(Abstract):
采用粉末包埋法对G115和T92钢表面进行低温渗铝,测试了两者渗铝前后在高温水蒸汽环境下的氧化行为。结果表明,在660℃水蒸汽环境下,G115钢的抗氧化性能优于T92钢;G115与T92钢表面制备的FeAl渗层具有优秀的抗高温水蒸汽氧化性能。同等实验条件下,渗铝试样的氧化增重比无渗层试样低两个数量级;G115钢中W、Cu等元素有利于渗层在高温水蒸汽中的稳定,可以有效地降低Al的扩散速率。
关键词(KeyWords): G115钢;T92钢;FeAl渗层;低温渗铝;高温氧化
基金项目(Foundation):
作者(Author): 董猛,谢逍原,朱阳存,杨淑莉,刘光明,汪元奎
DOI: 10.13289/j.issn.1009-6264.2020-0418
参考文献(References):
- [1] Zhang Y,Pint B A,Garner G W,et al.Effect of cycle length on the oxidation performance of iron aluminide coatings[J].Surface and Coatings Technology,2004,188:35-40.
- [2] Zhang Y,Liu A P,Pint B A.Interdiffusional degradation of oxidation-resistant aluminide coatings on Fe-base alloys[J].Materials and Corrosion,2007,58(10):751-761.
- [3] 屈文娟.1Cr11MoNiW1VNbN不锈钢Al-Si涂层组织结构及抗高温氧化性能研究[D].哈尔滨:哈尔滨工程大学,2011.QU Wen-juan.Research on microstruture and high-temperature oxidation property of Al-Si coating on 1Cr11MoNiW1VNbN stainless steel [D].Harbin:Harbin Engineering University,2011.
- [4] Agüero A,González V,Gutiérrez M,et al.Oxidation under pure steam:Cr based protective oxides and coatings[J].Surface and Coatings Technology,2013,237:30-38.
- [5] 刘正东,包汉生,徐松乾,等.用于超600 ℃蒸汽参数超超临界火电机组的新型马氏体G115耐热钢及其钢管研制[C]//2015年全国高品质特殊钢生产技术交流研讨会,中国金属学会,2015.
- [6] Xiao B,Xu L Y,Zhao L,et al.Transient creep behavior of a novel tempered martensite ferritic steel G115[J].Materials Science and Engineering A,2018,716:284-295.
- [7] 朱阳存,刘光明,董猛,等.T91钢表面低温渗层的动力学行为[J].材料热处理学报,2018,39(10):93-98.ZHU Yang-cun,LIU Guang-ming,DONG Meng,et al.Study on the dynamic behavior of low temperature aluminized layer on T91 steel surface[J].Transactions of Materials and Heat Treatment,2018,39(10):93-98.
- [8] 高海燕,贺跃辉,沈培智.FeAl金属间化合物研究现状[J].材料导报,2008,22(7):68-71.GAO Hai-yan,HE Yue-hui,SHEN Pei-zhi.Research status of FeAl intermet allics compound[J].Materials Review,2008,22(7):68-71.
- [9] 韦航标,王宇,李文川,等.P110钢表面韧性FeAl渗层的低温制备[J].材料热处理学报,2011,32(S1):166-169.WEI Hang-biao,WANG Yu,LI Wen-chuan,et al.Preparation of FeAl coating on P110 steel at low temperature[J].Transactions of Materials and Heat Treatment,2011,32(S1):166-169.
- [10] 胡德林.粉末低温渗铝的研究[J].金属热处理,1990(12):14-18.HU De-lin.Study on low temperature powder calorizing[J].Heat Treatment of Metals,1990(12):14-18.
- [11] 王静静,周云龙.过热器再热器爆漏事故的原因分析及对策[J].应用能源技术,2010(6):33-36.WANG Jing-jing,ZHOU Yun-long.Cause and analysis on superheater and reheater tube explosion and its countermeasures[J].Applied Energy Technology,2010(6):33-36.
- [12] Shigeta J,Hamao Y,Aoki H,et al.Development of a coal ash corrosivity index for high temperature corrosion[J].Journal of Engineering Materials and Technology,1987,109(4):299-305.
- [13] 张伟,刘爱萍,文九巴.镀铝温度对渗铝层/基体界面空洞生长动力学的影响[J].材料热处理学报,2012,33(4):127-131.ZHANG Wei,LIU Ai-ping,WEN Jiu-ba.Effects of aluminized temperature on the growth kinetics of voidsalong interface between aluminized layer and steel substrate[J].Transactions of Materials and Heat Treatement,2012,33(4):127-131.
- [14] 白银,陈正宗,刘正东,等.蒸汽温度对G115钢氧化行为的影响[J].钢铁研究学报,2020,32(1):52-59.BAI Yin,CHEN Zheng-zong,LIU Zheng-dong,et al.Effect of temperature on steam oxidation behavior of G115 steel[J].Journal of Iron and Steel Research,2020,32(1):52-59.
- [15] Pantip A,Gary S W.Oxidation of ferritic-martensitic alloys T91,HCM12A and HT-9 in supercritical water[J].Journal of Nuclear Materials,2007,371(1):1-17.
- [16] 高文华,沈朝,张乐福.T91钢在超临界水环境中的腐蚀性能[J].腐蚀与防护,2016,37(6):444-448.GAO Wen-hua,SHEN Zhao,ZHANG Le-fu.Corrosion behavior of T91 steel in supercritical water[J].Corrosion and Protection,2016,37(6):444-448.
- [17] Nishimuran,Komain,Hirayamay,et al.Japanese experience with steam oxidation of advanced heat-resistant steel tubes in power boilers[J].Materials at High Temperatures,2005,22 (1/2):3-10.
- [18] Steiner H,Konys J.Stresses in oxidized claddings and mechanical stability of oxide scales [M].FZKA,2006.
- [19] Pint B A,Zhang Y,Walker L R,et al.Long-term performance of aluminide coatings on Fe-base alloys[J].Surface and Coatings Technology,2007,202(4):637-642.
- [20] Agüero A,Muelas R.Steam oxidation of slurry aluminide coatings on ferritic steels for advanced coal-fired steam power plants[J].Materials Science Forum,2004(461/464):957-964.
- [21] Mogire E O,Higginson R L,Fry A T,et al.Microstructural characterization of oxide scales formed on steels P91 and P92[J].Materials at High Temperatures,2011,28(4):361-368.
- [22] Zhou Y H,Wang L,Wang G,et al.Influence of substrate composition on the oxidation performance of nickel aluminide coating prepared by pack cementation[J].Corrosion Science,2016,110:284-295.
- [23] 刘亚梅.9%Cr热强钢焊接金属时效微观组织与力学性能研究[D].秦皇岛:燕山大学,2015.LIU Ya-mei.Study on microstructure and mechanical properties of 9%Cr ferrite heat-resistant steel weld metal after aging [D].Qinhuangdao:Yanshan University,2015.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||