热处理工艺对S31042奥氏体耐热钢显微组织和力学性能的影响Effect of heat treatment on microstructure and mechanical properties of S31042 austenite heat resistant steel
杨征,赵新宝,张醒兴,党莹樱,鲁金涛,袁勇
摘要(Abstract):
研究S31042奥氏体耐热钢不同热处理工艺后的显微组织和力学性能。结果表明:随着时效温度由700℃上升到900℃,该钢的晶界M_(23)C_6型碳化物析出量增多,并逐渐呈现连续分布,冲击韧性显著降低,高温抗拉强度逐渐降低,屈服强度基本保持稳定,但900℃时效热处理后屈服强度略微增加;当时效温度由900℃上升到1000℃,该钢晶界碳化物析出量减少;高温抗拉强度变化不明显,屈服强度有所降低,冲击韧性提高;相比于拉伸过程中的低应变速率,在瞬时冲击高应变速率条件下,晶界M_(23)C_6相的聚集析出造成沿晶开裂倾向增加。
关键词(KeyWords): S31042钢;热处理;显微组织;力学性能
基金项目(Foundation): 华能国际电力股份有限公司科技项目(HNKJ17-H10);; 西安热工研究院有限公司科技项目(ZD-15-TYK07)
作者(Author): 杨征,赵新宝,张醒兴,党莹樱,鲁金涛,袁勇
DOI: 10.13289/j.issn.1009-6264.2017-0431
参考文献(References):
- [1]Beer J M.High efficiency electric power generation:the environmental role[J].Progress in Energy&Combustion Science,2007,33(2):107-134.
- [2]刘永坤,李成.我国能源效率及其影响因素分析[J].热力发电,2015(3):1-7.LIU Yong-kun,LI Cheng.China's energy efficiency and its influencing factors[J].Thermal Power Generation,2015,44(3):1-7.
- [3]Msuyama F.History of power plants and progress in heat resistant steels[J].ISIJ International,2007,41(6):612-625.
- [4]王崇斌,徐雪元,诸育枫,等.主蒸汽温度700℃超超临界锅炉水冷壁选材分析[J].热力发电,2015(7):66-71.WANG Chong-bin,XU Xue-yuan,CHU Yu-feng,et al.Material selection for water wall of ultra supercritical unit boilers with steam temperature of 700℃[J].Thermal Power Generation,2015,44(7):66-71.
- [5]Igarashi M.25Cr-20Ni-Nb-N Steel[M].Berlin:Springer Berlin Heidelberg,2004.
- [6]Iseda A,Okada H,Semba H,et al.Long term creep properties and microstructure of SUPER304H,TP347HFG and HR3C for AUSC boilers[J].Energy Materials Materials Science&Engineering for Energy Systems,2007,2(4):199-206.
- [7]Dudziak T,ukaszewicz M,Simmas N,et al.Steam oxidation of TP347HFG,Super 304H and HR3C-analysis of significance of steam flowrate and specimen surface finish[J].Corrosion Engineering Science&Technology,2015,50(4):272-282.
- [8]Komai N,Igarashi M,Minami Y,et al.Field test results of newly developed austenitic steels in the eddystone unit No.1 boiler[C]∥ASME 2007 Pressure Vessels and Piping Conference,2007:203-209.
- [9]杜宝帅,魏玉忠,张忠文,等.高温服役4.2万小时超超临界机组用HR3C钢组织与性能[J].材料热处理学报,2014,35(12):84-89.DU Bao-shuai,WEI Yu-zhong,ZHANG Zhong-wen,et al.Microstructure and properties of HR3C steel used in ultra-supercritical units after 42000 h exposure to elevated temperature[J].Transactions of Materials and Heat Treatment,2014,35(12):84-89.
- [10]彭志方,任文,杨超,等.HR3C钢运行过热器管的脆化与晶界M23C6相参量演化的关系[J].金属学报,2015,51(11):1325-1332.PENG Zhi-fang,REN Wen,YANG Chao,et al.The relationship between the evolution of phase parameters of grain Boundary M23C6and the embrittlement of HR3C super-heater tubes in service[J].Acta Metallurgica Sinica,2015,51(11):1325-1332.
- [11]欧梅桂,杨春林,杨祖建.热处理工艺对高温合金GH2132力学性能的影响[J].金属热处理,2014(6):91-93.OU Mei-gui,YANG Chun-lin,YANG Zu-jian.Effect of heat treatment on mechanical properties of high temperature alloy GH2132[J].Heat Treatment of Metals,2014,39(6):91-93.
- [12]Du J H,Lu X D,Deng Q.Effect of heat treatment on microstructure and mechanical properties of GH4169 superalloy[J].Rare Metal Materials&Engineering,2014,43(8):1830-1834.
- [13]于秋颖,董建新,张麦仓,等.热处理制度对超超临界电站用GH80A合金组织和性能的影响[J].稀有金属材料与工程,2013,42(7):1507-1512.YU Qiu-ying,DONG Jian-xin,ZHANG Mai-cang,et al.Influence of heat treatments on microstructures and properties of GH80A superalloy for buckets of USC steam turbines[J].Rare Metal Materials and Engineering,2013,42(7):1507-1512.
- [14]王斌,刘正东,程世长,等.固溶处理工艺对HR3C奥氏体耐热钢组织和性能的影响[J].机械工程材料,2014,38(6):25-30.WANG Bin,LIU Zheng-dong,CHENG Shi-chang,et al.Effect of solid solution treatment on microstructure and mechanical properties of HR3C austenite heat resistant steel[J].Material for Mechanical Engeering,2014,38(6):25-30.
- [15]Yan J,Gu Y,Sun F,et al.Evolution of microstructure and mechanical properties of a 25Cr-20Ni heat resistant alloy after long-term service[J].Materials Science and Engineering A,2016,675:289-298.
- [16]方圆圆,赵杰,李晓娜.HR3C钢高温时效过程中的析出相[J].金属学报,2010,46(7):844-849.FANG Yuan-yuan,ZHAO Jie,LI Xiao-na.Precipitates in HR3C steel aged at high temperature[J].Acta Metallurgica Sinica,2010,46(7):844-849.
- [17]王敬忠,刘正东,程世长,等.固溶态S31042钢高温塑性波动大的原因分析[J].钢铁,2012,47(1):60-64.WANG Jing-zhong,LIU Zheng-dong,CHENG Shi-chang,et al.Analysis on big fluctuation in elevated temperature ductility of solution S31042 steel[J].Iron and Steel,2012,47(1):60-64.
- [18]Wang B,Liu Z D,Cheng S C,et al.Microstructure evolution and mechanical properties of HR3C steel during long-term aging at high temperature[J].Journal of Iron and Steel Research,International,2014,21(8):765-773.
- [19]郑子杰.HR3C钢管时效冲击韧性大幅降低的原因分析[J].锅炉技术,2011,42(4):46-48.ZHENG Zi-jie.The analysis of considerably reduction to HR3C’s aging impact ductility[J].Bolier Technology,2011,42(4):46-48.
- [20]Zhang Z,Hu Z,Tu H,et al.Microstructure evolution in HR3C austenitic steel during long-term creep at 650℃[J].Materials Science&Engineering A,2016,681:74-84.
- [21]Zhao J,Wang H,Cheng C Q,et al.Precipitation in 25Cr20Ni Nb N austenitic steel after ageing at 750℃[J].Materials at High Temperatures,2015,32(5):461-467.
- [22]Wang J Z,Liu Z D,Bao H S,et al.Evolution of precipitates of S31042 heat resistant steel during 700℃aging[J].Journal of Iron and Steel Research,International,2013,20(10):113-121.
- [23]侯本睿,赵新宝,杜双明,等.短期时效处理对HR3C合金显微组织和显微硬度的影响[J].热加工工艺,2016(18):245-248.HOU Ben-rui,ZHAO Xin-bao,DU Shuang-ming,et al.Effect of short-Aging treatment on microstructure and micro-hardness of HR3C alloy[J].Hot Working Technology,2016,(18):245-248
- [24]Peng B,Zhang H,Hong J,et al.Effect of aging on the impact toughness of 25Cr-20Ni-Nb-N steel[J].Materials Science and Engineering A,2010,527(7):1957-1961.
- [25]Futamura Y,Tsuchiyama T,Takaki S.Strengthening mechanism of Cu bearing heat resistant martensitic steels[J].ISIJ International,2007,41(S):477-482.
- [26]亨利G,豪斯特曼D.宏观断口学及显微断口学[M].北京:中国机械工业出版社,1990.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||