应变速率和变形量对合金元素在Ti3Al和TC11焊接界面上扩散的影响Effects of strain rate and deformation amount on diffusion of alloying elements at Ti3Al and TC11 welding interface
刘莹莹,姚泽坤,郭鸿镇
摘要(Abstract):
研究了Ti3Al基合金与TC11钛合金采用不同参数的电子束焊接的双合金件,经近等温锻造和热处理后,近等温锻造工艺参数对合金元素在焊接界面上扩散的影响。结果表明,应变速率和变形量对不同参数焊接的双合金件焊接界面合金元素扩散的影响类似,均随着应变速率的降低及变形量的增大扩散更充分。但当变形20%时,合金元素以沿晶界扩散的管道机制为主;当变形40%时,扩散以晶间扩散机制为主。此外,Ti元素在焊缝区的反常扩散是由于Ti原子的点阵位置被从Ti3Al侧扩散而来的Nb原子所占据,被替代的Ti原子从DO19六方有序结构中扩散出来聚集所造成。
关键词(KeyWords): Ti3Al;TC11;焊接界面;应变速率;变形量;元素扩散
基金项目(Foundation): 国家自然科学基金资助项目(50775187)
作者(Author): 刘莹莹,姚泽坤,郭鸿镇
DOI: 10.13289/j.issn.1009-6264.2010.01.022
参考文献(References):
- [1]Fukumoto S,Inuki T,Tsubakino H,et al.Evaluation of friction weld interface of aluminium to austenitic stainless steel joint[J].Materials Scienceand Technology,1997,13:679-686.
- [2]Bell R A,Lippold J C,Adolphson D R.An evaluation of copper-stainless inertia friction welds[J].Welding Journal.1984,63(11):325s-332s.
- [3]Mourer P,Raymond E,Ganesh S,et al.Dual alloy disk development[C].Superalloys 1996.Warrendale,TMS,1996:637-643.
- [4]Yao Z K,Guo HZ,Cui Z S,et al.The influence of hot working processing on mechanical properties of Ti3Al-Ti dual alloy welded by electronicbeam welding in vacuum[C].Proceeding of the 10th World conference on Titanium,Warrendale,TMS,2004:715-720.
- [5]姚泽坤,张梅琳,梁新民,等.热力耦合作用对TAC-1B和TC11合金焊接界面硬度和显微组织的影响[J].焊接学报,2004,25(2):125-129.YAO Ze-kun,ZHANG Mei-lin,LIANG Xin-min,et al.Influence of heat and force coupling action on micro-hardness and microstructures at weldseam of TAC-1B/TC11 alloy[J].Transactions of the China Welding Institution,2004,25(2):125-129.
- [6]Yao Z K,Liang X M,Guo HZ,et al.The influence of processing parameters on mechanical properties and microstructure of welding zone for Ti3Al-TC4 dual alloy[C].The fifth Rim International Conference on Advanced Materials and Processing.Warrendale:TMS,2004:445-448.
- [7]姚泽坤,梁新民,郭鸿镇,等.热力因素对合金元素Ti-24Al-15Nb-1.5Mo/TC4焊接界面上扩散规律的影响研究[J].稀有金属材料与工程,2005,34(6):907-911.YAO Ze-kun,LIANG Xin-min,GUO Hong-zhen,et al.Effect of hot and force factors on the microhardness and elements diffusion at Ti3Al/TC4seam[J].Rare Metal Materials and Engineering,2005,34(6):907-911.
- [8]刘莹莹,姚泽坤,罗茜,等.Ti-24Al-15Nb-1.5Mo合金的超塑性能及超塑变形时的组织演化[J].稀有金属材料与工程,2008,37(1):14-18.Liu Y Y,Yao Z K,Luo X,et al.Superplastic properties and microstructural evolution during superplastic tension of Ti-24Al-15Nb-1.5Mo alloy[J].Rare Metal Materials and Engineering,2008,37(1):14-18.
- [9]张立斌,白秉哲,戴积林,等.TC11压气机盘超塑等温锻造工艺[J].航天工艺,1996(4):38-41.
- [10]Xu D S,Song Y,Li D,et al.Site occupancy of alloying elements in Ti3Al compounds[J].Materials Science and Engineering A,1997,234-236:230-233.
- [11]Hao Y L,Xu D S,Cui YY,et al.The site occupancies of alloying elements in TiAl and Ti3Al alloys[J].Acta Materialia,1999,47:1129-1139.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||