直接Q&P处理超高强钢的组织与力学性能Microstructure and mechanical properties of an ultra high strength steel after direct quenching and partitioning process
万德成,陈雨来,蔡庆伍
摘要(Abstract):
为了改善超高强钢的塑韧性,采用轧后直接淬火到马氏体区等温配分的工艺,研究配分时间对中碳低合金超高强钢组织和力学性能的影响规律。结果表明:在260℃等温配分处理,钢的组织包括初生马氏体、新生马氏体和残留奥氏体,在等温过程中还有碳化物析出和等温马氏体形成。在等温配分过程中,碳由马氏体向奥氏体扩散处于主导地位,残留奥氏体含量不断增加,新生马氏体量减少,塑性和韧性提高。等温配分后期,由于碳化物不断析出消耗碳原子,导致扩散到奥氏体中的碳原子减少,残留奥氏体体积分数增加缓慢。析出相粒子在等温过程中没有明显长大,起到了抵抗马氏体软化的作用。等温60 min具有良好的强度和塑韧性能,抗拉强度1546 MPa、伸长率为15.3%,-20℃冲击功为27.5 J。
关键词(KeyWords): 超高强钢;配分工艺;组织;力学性能;残留奥氏体
基金项目(Foundation):
作者(Author): 万德成,陈雨来,蔡庆伍
DOI: 10.13289/j.issn.1009-6264.2014.05.026
参考文献(References):
- [1]徐祖耀.自主创新发展超高强度钢[J].上海金属,2009,31(2):1-5.XU Zu-yao.Self-reliance innovation on development of ultra-high strength steel[J].Shanghai Metals,2007,22(1):1-5.
- [2]徐祖耀.马氏体与马氏体相变[M].北京:科学出版社,1988.
- [3]Sugimoto K,Misu M,Kobayashi M,Shirasawa H.Effects of second phase morphology on retained austenite morphology and tensile properties in a TRIP-aided dual-phase steel sheet[J].ISIJ International,1993,33(7):775-782.
- [4]Garcia-Mateo C,Caballero F G,Chao J,et al.Mechanical stability of retained austenite during plastic deformation of super high strength carbide free bainitic steels[J].Journal of Materials Science,2009,44(17):4617-4624.
- [5]Speer J G,Matlock D K,De Cooman B C,et al.Carbon partitioning into austenite after martensite transformation[J].Acta Materialia,2003,51(9):2611-2622.
- [6]Matlock D K,Brutigam V E,Speer J G.Application of the quenching and partitioning(Q&P)process to a medium-carbon,high Si microalloyed bar steel[J].Materials Science Forum,2003,426-432:1089-1094.
- [7]Speer J G,Rizzo F C,Matlock D K,et al.The“quenching and partitioning”process:background and recent progress[J].Materials Research,2005,8(4):417-423.
- [8]庄宝潼,唐荻,江海涛,等.Q&P工艺对0.3C-1.35Mn-1.30Si钢力学性能的影响[J].材料热处理学报,2011,32(11):34-38.ZHUANG Bao-tong,TANG Di,JIANG Hai-tao,et al.Influence of quenching and partitioning process on mechanical properties of a 0.3C-1.35Mn-1.30Si steel[J].Transactions of Materials and Heat Treatment,2011,32(11):34-38.
- [9]Zhou S,Zhang K,Wang Y,et al.High strength-elongation product of Nb-microalloyed low-carbon steel by a novel quenching-partitioning-tempering process[J].Materials Science and Engineering A,2011,528(27):8006-8012.
- [10]王建军,焦贵鹏,刘沿东,等.Q&P热处理工艺对C-Si-Mn钢组织性能的影响[J].材料热处理学报,2013,34(3):104-107.WANG Jian-jun,JIAO Gui-peng,LIU Yan-dong,et al.Influence of quenching and partitioning process on microstructure and properties of a C-Si-Mn steel[J].Transactions of Materials and Heat Treatment,2013,34(3):104-107.
- [11]Kaputkin D E,Kaputkina L M,Prokoshkin S D.Transformation of retained austenite during tempering of high carbon steel[J].Journal de Physique IV,2003,112(1):275-278.
- [12]王立军,蔡庆伍,余伟,等.1500MPa级低合金超高强度钢的微观组织与力学性能[J].金属学报,2010,46(6):687-694.WANG Li-jun,CAI Qing-wu,YU Wei,et al.Microstructure and mechanical properties of 1500MPa grade ultra-high strength low alloy steel[J].Acta Metallurgica Sinica,2010,46(6):687-694.
- [13]Kim D,Speer J G,De Cooman B C.Isothermal transformation of a CMnSi steel below the Ms temperature[J].Metallurgical and Materials Transactions A,2011,42(6):1575-1585.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||