工艺参数对原位合成WCP增强铁基复合材料的影响Effect of process parameters on in-situ synthesis of WCP/Fe composites
牛立斌,王晓刚,樊子民
摘要(Abstract):
以金属钨丝网和灰口铸铁为原材料,采用离心铸造技术,通过调整钨丝的中心间距和灰口铸铁熔体的浇铸温度,原位合成WC颗粒增强铁基复合材料。利用XRD、SEM以及两体销盘磨损试验机对所得复合材料复合区的物相种类、显微组织以及磨损性能进行分析研究,结果表明:随浇铸温度的提高,WC衍射峰的强度增强,反应程度增大,WC量不断增多。当钨丝中心间距为0.5 mm,浇铸温度为1400℃时,得到较理想的WC颗粒弥散分布于铁基体中的复合材料;在浇铸温度不变时,随中心距的增大,复合材料的磨损率呈现出先降低后略微升高的趋势。
关键词(KeyWords): 复合材料;碳化钨;原位合成;磨损
基金项目(Foundation): 国家自然科学基金(50174046);; 陕西省科技统筹计划项目(KTCQ1-17);; 西安市技术转移工程项目(CX1261)
作者(Author): 牛立斌,王晓刚,樊子民
DOI: 10.13289/j.issn.1009-6264.2014.03.005
参考文献(References):
- [1]LI Zu-lai,JIANG Ye-hua,ZHOU Rong,et al.Dry three-body abrasive wear behavior of WC reinforced iron matrix surface composites produced by VEPC infiltration casting process[J].Wear,2007(5-6),262:649-654.
- [2]隋育栋,蒋业华,李祖来,等.WC溶解对WCp/钢基表层复合材料组织和性能的影响[J].材料热处理学报,2012,33(S):7-10.SUI Yu-dong,JIANG Ye-hua,LI Zu-lai,et al.Effects of WC dissolute in matrix on microstructure and properties of WC reinforced steel composite[J].Transactions of Materials and Heat Treatment,2012,33(S):7-10.
- [3]LI Ye-fei,GAO Yi-min.Three-body abrasive wear behavior of CC/high-Cr WCI composite and its interfacial characteristics[J].Wear,2010,268(3-4):511-518.
- [4]朱流,郦剑.WC-10%Co激光熔覆涂层的制备及耐磨性能[J].机械工程材料,2008,32(8):26-29.ZHU Liu,LI Jian.Preparation and wear-resistance of WC-10%Co laser cladded layer[J].Materials for Mechanical Engineering,2008,32(8):26-29.
- [5]袁有录,李铸国.等离子熔覆WC-Ni/Fe梯度涂层的组织与性能[J].材料热处理学报,2012,33(11):131-136.YUAN You-lu,LI Zhu-guo.Microstructure and properties of WC-Ni/Fe grandient coating on Q235 steel formed by plasma cladding[J].Transactions of Materials and Heat Treatment,2012,33(11):131-136.
- [6]Do Nascimento,Ocelik A.M,et al.Microstructure of reaction zone in WCp/duplex stainless steels matrix composites processing by laser melt injection[J].Surface and Coatings Technology,2008,202(10):2113-2120.
- [7]李松林,向锦涛,周伍喜,等.超音速火焰喷涂WC-10Co4Cr涂层的耐滑动磨损行为[J].中国有色金属学报,2012,22(5):1371-1376.LI Song-lin,XIANG Jin-tao,ZHOU Wu-xi,et al.Sliding wear behavior of high-velocity oxy-fuel sprayed WC-10Co4Cr coatings[J].The Chinese Journal of Nonferrous Metal,2012,22(5):1371-1376.
- [8]Wang H Y,Jiang Q C,Li X L,et al.In situ synthesis of TiC/Mg composites in molten magnesium[J].Scripta Mater,2003,48(9):1349-1354.
- [9]刘丽,刘慧敏,张复懿.原位TiC颗粒含量对近液相线铸造7075铝合金二次加热组织的影[J].中国有色金属学报,2010,20(2):233-238.LIU Li,LIU Hui-min,ZHANG Fu-yi.Effect of in-situ TiC concentration on reheating microstructure of near-liquidus cast 7075 A1 alloy[J].The Chinese Journal of Nonferrous Metals,2010,20(2):233-238.
- [10]Ali Emamian,Stephen F.Corbin,Amir Khajepour.Effect of laser cladding process parameters on clad quality and in-situ formed microstructure of FeTiC composite coatings[J].Surface and Coatings Technology,2010,205(7):2007-2015.
- [11]柴禄,李惠琪,姬强,等.原位冶金反应碳化钨增强铁基复合材料[J].材料热处理学报,2012,33(S):33-36.CHAI Lu,LI Hui-qi,JI Qiang,et al.Fe-based composite reinforced with WC particles prepared by in-situ metallurgy reaction[J].Transactions of Materials and Heat Treatment,2012,33(S):33-36.
- [12]NIU Li-bin,XU Yun-hua,WU Hong,et al.Preparation of In-situ(Fe,Cr)7C3/Fe composite coating by centrifugal casting[J].Surface Engineering,2010,3:675-680.
- [13]Antoni,Zdziobek A,Shen J Y,et al.About one stable and three metastable eutectic microconstituents in the Fe-W-C system[J].International Journal of Refractory Metals&Hard Materials,2008,26(4):372-382.
- [14]Kurt B,Orhan N,Hascalk A.Effect of high heating and cooling rate on interface of diffusion bonded gray cast iron to medium carbon steel[J].Materials and Design,2007,28(7):2229-2233.
- [15]Cree D,Pugh M.Dry Wear and friction properties of an A356/SiC foam interpenetrating phase composite[J].Wear,2011,272(1):88-96.
- [16]ZHOU Rong,JIANG Ye-hua,LU De-hong.The effect of volume fraction of WC particles on erosion resistance of WC reinforced iron matrix surface composites[J].Wear,2003,255(1-6):134-138.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||