IN740H镍基高温合金的应力腐蚀性能Stress corrosion properties of IN740H nickel-base superalloy
李冬升,凌瀚宇,王威,刘勇,刘仁才
摘要(Abstract):
采用慢速应变速率应力腐蚀试验研究了高盐环境对IN740H镍基高温合金应力腐蚀行为的影响。结果表明:在近中性3 mol/L NaCl溶液和酸性2.5 mol/L NaCl+0.5 mol/L HCl溶液中,IN740H镍基高温合金的应力腐蚀敏感性系数均小于25%,没有发生应力腐蚀,仅存在一定的应力腐蚀断裂倾向;合金在酸性2.5 mol/L NaCl+0.5 mol/L HCl溶液中表现出最高的应力腐蚀敏感性,并且慢应变速率拉伸(SSRT)断口表现为脆性和韧性断裂的混合断裂方式,说明IN740H镍基高温合金在高盐环境下仍有较好的抗应力腐蚀性能。
关键词(KeyWords): IN740H镍基高温合金;NaCl;HCl;慢应变速率;应力腐蚀
基金项目(Foundation):
作者(Author): 李冬升,凌瀚宇,王威,刘勇,刘仁才
DOI: 10.13289/j.issn.1009-6264.2022-0387
参考文献(References):
- [1] 方安千,芦敬安,冀晋川.在超(超)临界机组中应用的新钢种[J].山西电力,2009(4):56-60.FANG An-qian,LU Jing-an,JI Jin-chuan.Application of new types of steel in ultra-supercritical unit[J].Shanxi Electric Power,2009(4):56-60.
- [2] 朱全利.锅炉设备及系统[M].北京:中国电力出版社,2006:1-5.
- [3] 赖洪彬.660MW燃煤发电机组高效脱硫提效改造技术的应用[J].化学工程与装备,2019(7):315-317.LAI Hong-bin.Application of high efficiency desulfurization and efficiency improvement technology for 660MW coal-fired generating units[J].Chemical Engineering & Equipment,2019(7):315-317.
- [4] 赵凯.燃煤发电机组锅炉宽负荷脱硝的研究与应用[J].资源节约与环保,2017(8):21-23.ZHAO Kai.Research and application of denitration in coal-fired generator boiler under wide load[J].Resources Economization & Environmental Protection,2017(8):21-23.
- [5] 李庆春,张虔,郝维勋,等.电站锅炉不锈钢部件的制造过程防护[J].锅炉制造,2021(6):45-46.LI Qing-chun,ZHANG Qian,HAO Wei-xun,et al.Manufacturing process protection of stainless steel parts for utility boilers[J].Boiler Manufacturing,2021(6):45-46.
- [6] 林富生,谢锡善,赵双群,等.我国700 ℃超超临界锅炉过热器管用高温合金选材探讨[J].动力工程学报,2011,31(12):960-968.LIN Fu-sheng,XIE Xi-shan,ZHAO Shuang-qun,et al.Selection of superheater tubes of domestic 700 ℃ A-USC boilers[J].Chinese Journal of Power Engineering,2011,31(12):960-968.
- [7] 曾凡博,李宏,吴青松,等.热处理工艺对700 ℃以上超超临界电站用镍基合金组织及性能的影响[J].钢管,2018,47(2):21-25.ZENG Fan-bo,LI Hong,WU Qing-song,et al.Effect of heat treatment process on microstructure and properties of nickel base alloy for ultra supercritical power station above 700 ℃[J].Steel Pipe,2018,47(2):21-25.
- [8] 赵双群,张麦仓,董建新,等.新型高温合金700 ℃时效组织及力学性能[J].稀有金属材料与工程,2003,32(12):991-994.ZHAO Shuang-qun,ZHANG Mai-cang,DONG Jian-xin,et al.Mechanical properties and structure of new superalloys after prolonged aging at 700 ℃[J].Rare Metal Materials and Engineering,2003,32(12):991-994.
- [9] 赵双群,谢锡善.超超临界锅炉过热器管材的高温组织稳定性及其改进研究[J].材料导报,2004,18(8):131-133.ZHAO Shuang-qun,XIE Xi-shan.High temperature structure stability and its improvement on superheater tube material for ultra-supercritical boilers[J].Materials Review,2004,18(8):131-133.
- [10] 张红军,周荣灿,侯淑芳,等.先进超超临界机组用Inconel 740合金的组织稳定性研究[J].中国电机工程学报,2011,31(8):108-113.ZHANG Hong-jun,ZHOU Rong-can,HOU Shu-fang,et al.Study on microstructure stability of Inconel 740 for advanced ultra supercritical unit[J].Proceedings of the CSEE,2011,31(8):108-113.
- [11] 张红军,周荣灿,侯淑芳,等.先进超超临界机组用Inconel 740合金的组织稳定性研究[J].中国电机工程学报,2011,31(8):108-113.ZHANG Hong-jun,ZHOU Rong-can,HOU Shu-fang,et al.Study on microstructure stability of Inconel 740 alloy for advanced ultra supercritical unit[J].Proceedings of the CSEE,2011,31(8):108-113.
- [12] 赵双群,谢锡善,董建新.Inconel 740合金在空气和含有水蒸气的空气中的氧化研究[J].动力工程学报,2011,31(10):797-802.ZHAO Shuang-qun,XIE Xi-shan,DONG Jian-xin.Oxidation of Inconel 740 alloy in air and air containing water vapor[J].Chinese Journal of Power Engineering,2011,31(10):797-802.
- [13] 符锐,林富生,赵双群,等.Inconel 740H主要强化元素对热力学平衡相析出行为的影响[J].动力工程学报,2013,33(5):405-412.FU Rui,LIN Fu-sheng,ZHAO Shuang-qun,et al.Effect of main strengthening elements of Inconel 740H on precipitation behavior of thermodynamic equilibrium phase[J].Chinese Journal of Power Engineering,2013,33(5):405-412.
- [14] 郭岩,李太江,王彩侠,等.镍基合金740H时效过程中的显微组织与相析出行为[J].中国有色金属学报(英文版),2016,26(6):1598-1606.GUO Yan,LI Tai-jiang,WANG Cai-xia,et al.Microstructure and phase precipitation behavior of nickel base alloy 740H during aging[J].Transactions of Nonferrous Metals Society of China,2016,26(6):1598-1606.
- [15] 郭岩,周荣灿,张红军,等.镍基合金740H的组织结构与析出相分析[J].中国电机工程学报,2015,35(17):4439-4444.GONG Yan,ZHOU Rong-can,ZHANG Hong-jun,et al.Microstructure and precipitates of alloy 740H[J].Proceedings of the CSEE,2015,35(17):4439-4444.
- [16] 高佩,朱海涛,程晓农,等.700 ℃超超临界锅炉用Inconel 740H合金的热塑性[J].金属热处理,2017,42(9):124-127.GAO Pei,ZHU Hai-tao,CHENG Xiao-nong,et al.Hot ductility of Inconel 740H alloy for 700 ℃ ultra supercritical boilers[J].Heat Treatment of Metals,2017,42(9):124-127.
- [17] 侯世香,吴正发,袁晓娜,等.Inconel 740H合金在模拟煤灰/烟气中的抗腐蚀性研究[J].腐蚀科学与防护技术,2016,28(3):247-252.HOU Shi-xiang,WU Zheng-fa,YUAN Xiao-na,et al.Corrosion resistance of 740H in simulated coal-ash/flue-gas environments[J].Corrosion Science and Protection Technology,2016,28(3):247-252.
- [18] 谢奕心,程晓农,徐桂芳,等.高温合金Inconel 740H在空气和水蒸气环境中的氧化行为[J].热加工工艺,2018,47(14):55-59.XIE Yi-xin,CHENG Xiao-nong,XU Gui-fang,et al.Oxidation behavior of high temperature alloy Inconel 740H in air and water vapor environment[J].Hot Working Technology,2018,47(14):55-59.
- [19] 党莹樱,赵新宝,尹宏飞,等.Inconel 740H蠕变过程中晶界M23C6的粗化行为[J].材料科学与工艺,2017,25(6):22-26.DANG Ying-ying,ZHAO Xin-bao,YI Hong-fei,et al.Coarsening behavior of grain boundary M23C6 in Inconel 740H during creep[J].Materials Science and Technology,2017,25(6):22-26.
- [20] 鲁金涛,谷月峰,杨珍.3种700 ℃级超超临界燃煤锅炉备选高温合金煤灰腐蚀行为[J].腐蚀科学与防护技术,2014,26(3):205-210.LU Jin-tao,GU Yue-feng,YANG Zhen.Coal ash induced corrosion of three candidate materials for superheater boiler tubes of advanced ultrasupercritical power station[J].Corrosion Science and Protection Technology,2014,26(3):205-210.
- [21] 范益,程焕林,李浩,等.NaCl和Na2S混合溶液pH对SA516Gr70N钢应力腐蚀开裂的影响[J].腐蚀与防护,2021,42(11):28-36.FAN Yi,CHENG Huan-lin,LI Hao,et al.Effect of pH on SCC behavior of SA516Gr70N steel in NaCl/Na2S solution[J].Corrosion & Protection,2021,42(11):28-36.
- [22] 鲁金涛,杨珍,徐松乾,等.Inconel 740H合金在纯水蒸气环境中的高温氧化行为[J].机械工程材料,2015,39(10):37-41.LU Jin-tao,YANG Zhen,XU Song-qian,et al.High temperature oxidation behavior of Inconel 740H alloy in pure steam[J].Materials for Mechanical Engineering,2015,39(10):37-41.
- [23] 王晋,张跃飞,马晋遥,等.Inconel 740H合金原位高温拉伸微裂纹萌生扩展研究[J].金属学报,2017,53(12):1627-1635.WANG Jin,ZHANG Yue-fei,MA Jin-yao,et al.Microcrack nucleation and propagation investigation of Inconel 740H alloy under in situ high temperature tensile test[J].Acta Metallurgica Sinica,2017,53(12):1627-1635.
- [24] 杨世洲,李春福,李辉,等.饱和H2S环境下慢应变速率对2205双相不锈钢应力腐蚀性能的影响[J].材料热处理学报,2016,37(11):96-102.YANG Shi-zhou,LI Chun-fu,LI hui,et al.Influence of slow strain rate on stress corrosion cracking of 2205 duplex stainless steel in saturated H2S environment[J].Transactions of Materials and Heat Treatment,2016,37(11):96-102.
- [25] Yu Q,Dong C F,Liang J X,Liu Z B,et al.Stress corrosion cracking behavior of PH13-8Mo stainless steel in Cl- solutions[J].Journal of Iron and Steel Research,International,2017,24(3):282-289.
文章评论(Comment):
|
||||||||||||||||||
|
||||||||||||||||||